Tshwj xeeb Alumina Cib

Tshwj xeeb alumina cib yog ua los ntawm qib siab sillimanite, pyrite, mullite, thiab corundum ua raw khoom, thiab muaj refractoriness ntawm 1750 ~ 1790 degree.
MOQ: 5 tons
Xa kev nug
Khoom Taw qhia
Kev piav qhia

 


Tshwj xeeb alumina cib muaj ntau Al2O3, uas yog ze rau nruab nrab cov ntaub ntawv refractory thiab tuaj yeem tiv taus cov kua qaub slag thiab alkaline slag. Ntawm lawv, Al2O3 yog siab, thiab tus nqi ntawm impurities yog me me, thiab tsim ntawm fusible iav yog me me. Yog li ntawd, lub load softening kub yog siab dua li cov av nplaum cib.

Tshwj xeeb alumina refractory cib tuaj yeem muab faib ua ntau hom raws li lawv cov khoom tshwj xeeb thiab kev siv. Piv txwv li, fireclay cib yog ib hom tshwj xeeb alumina cib uas muaj cov feem pua ​​​​ntawm cov av nplaum ntau dua thiab muaj cov thermal poob siab zoo, ua rau lawv zoo tagnrho rau kev siv hauv qhov cub tawg thiab cov ntawv siv hlau. Mullite bricks, ntawm qhov tod tes, muaj kev sib xyaw ntawm alumina thiab silica thiab siv rau hauv cov ntawv thov kub xws li cov kab hauv tsev thiab cov phab ntsa rauv.

 

Nta

 

Tshwj xeeb alumina cib yog ib hom refractory cib ua los ntawm high-purity alumina thiab lwm yam ntaub ntawv. Lawv yog tsim los tiv taus kub, corrosion, thiab puas nyob rau hauv ntau yam kev siv.

Kev ua tau zoo nyob rau hauv high temp refractoriness nyob rau hauv load / Siab kub resistant nrog zoo refractoriness

Cov ntsiab lus qis dua impurity / Zoo thermal poob siab kev ua haujlwm / Kev ua haujlwm zoo hauv slag abrasion

Zoo txias crush lub zog

 

Daim ntawv thov

 

Tshwj xeeb alumina cib yog tsuas yog siv rau hauv ob sab phlu blast furnaces, kub moj tej tawg rauv, hluav taws xob rauv lub ru tsev, blast furnaces, reverberatory furnaces, thiab teb kilns. Lawv yog cov khoom tseem ceeb hauv ntau cov txheej txheem kev lag luam uas yuav tsum muaj qhov kub thiab txias

 

Physical And Chemical Indicators

 

Hom
Cov khoom

TSI 80

TSI 75

TSI 70

SAL60

Refractoriness (SK)

39

39

38

37

Pom tseeb Porosity (%)

17

18

18

18

Qhov ceev (g / cm3)

2.75

2.65

2.65

2.50

Txias Crushing zog (MPa)

80

70

70

60

@ 1, 000 degree

Thermal Linear Expansion (%)

0.65

0.65

0.55

0.53

 @ 1,500qib x2h

Permanent Linear Change (%)

 

±0.2

±0.2

145 0 degree x2h ± 0.2

145 0 degree x2h ± 0.2

 @0.2MPa

Refractoriness Nyob rau hauv Load (degree)

1,670

1,650

1,600

1,580

Tshuaj

Kev sib xyaw (%)

Al2O3

80

76

70

60

Fe2O3

0.8

1.0

1.2

1.2

Cov ntawv thov tseem ceeb

Txiv qaub Kiln Cement Kiln
Ntau yam Rotary kiln
Iav melting TankElectric Arc FurnaceBlast Rauv
Chamber Combustor
Nonferrous Hlau Rauv
Ntau lub qhov cub kub