Khiav cib feem ntau yog siv hauv qab casting thiab pouring steel. Cov laj thawj uas cuam tshuam rau purity ntawm steel feem ntau muab faib ua ob pawg:
1. Nws yog tshwm sim los ntawm cov txheej txheem steelmaking;
2. Nws yog tshwm sim los ntawm cov ntaub ntawv refractory rau steelmaking, xws li ntws steel cib. Thaum molten steel ntws los ntawm lub molten steel tank mus rau ingot pwm, nws yuav tsum dhau los ntawm ntws steel cib. Vim lub siab kub ntawm cov hlau molten, cov ntws steel cib yuav raug cuam tshuam, uas yuav ua rau cov hlau ntws. Ib feem ntawm cov qauv steel cib poob, thiab tib lub sij hawm cov hlau molten yuav cuam tshuam nrog cov ntws steel cib, thiab cov khoom siv tshuaj tiv thaiv yuav muab sib xyaw rau hauv cov hlau molten, uas yuav cuam tshuam rau qhov zoo ntawm cov hlau ingot.
Kev khiav dej num zoo yuav tsum muaj cov dej ntws zoo ua haujlwm kom ntseeg tau tias cov dej uas nkag mus tau tuaj yeem nkag mus rau hauv dej hauv lub sijhawm thiab ua haujlwm tau zoo. Yog li ntawd, nws yog ib qho tseem ceeb uas yuav tsum tau siv cov ntaub ntawv cementitious tov nrog steel los yog txiv qaub li cov xuab zeb ntawm cov cam khwb cia steel cib.
1. Nws yuav tsum tau ntxuav nruab nrab coarse xuab zeb. Vim hais tias ntawm qhov yuav tsum tau ua ntej lub zog txwv, lub cev Performance index ntawm cov xuab zeb ntawm cam khwb cia steel cib cushion tsis tau teev nyob rau hauv no hais txog.Bedding yuav tsum tau rau khiav cib:
2. Lub cev lub cev ua haujlwm ntawm lwm cov txheej txheem ntawm cov hlau nplaum yuav tsum ua kom tau raws li qhov yuav tsum tau ua ntawm tus qauv.
3. Nws yuav tsum yog semi-qhuav xuab zeb. Txoj kev tswj cov av noo yog nyem qhov sib tov rau hauv ib pawg ntawm tes. Tau kawg, nws yuav dhau tom qab loosening. Qhuav thiab ntub dej yog qhov zoo rau kev ua kom lub ntsej muag, txo qhov ntom ntom ntawm Yang plua plav thiab txhawb nqa lub cushion.
Daim ntawv thov
Khiav cib yog siv rau hauv cov hlau ua blast furnaces, steel-ua converters, refining furnaces, hluav taws xob furnaces thiab lwm yam khoom siv ziab, muffle furnaces, thiab lwm yam.
Physical And Chemical Indicators
| Index/brand | N-1 | N-2a | N-2b | N-3a | N-3b | N-4 | N-5 | N-6 | |
| Refractoriness degree Ntau dua lossis sib npaug | 1750 | 1730 | 1730 | 1710 | 1710 | 1690 | 1670 | 1580 | |
| 0.2Mpa load softening pib kub siab dua los yog sib npaug rau | 1400 | 1350 | 1350 | 1320 | 1320 | 1300 | 1300 | 1300 | |
| Reburning kab hloov feem pua | 1400 degree 2 h | ntxiv rau 01-0.4 | ntxiv rau 01-0.5 | ntxiv rau 02-0.5 | ntxiv rau 02-0.5 | ntxiv rau 02-0.5 | ntxiv rau 02-0.5 | ntxiv rau 02-0.5 | ntxiv rau 02-0.5 |
| 1350 degree 2h | ntxiv rau 01-0.4 | ntxiv rau 01-0.5 | ntxiv rau 02-0.5 | ntxiv rau 02-0.5 | ntxiv rau 02-0.5 | ntxiv rau 02-0.5 | ntxiv rau 02-0.5 | ntxiv rau 02-0.5 | |
| Pom meej porosity feem pua Tsawg dua los yog sib npaug | 22 | 24 | 26 | 24 | 26 | 24 | 26 | 28 | |
| Ib txwm kub compressive zog Mpa degree Ntau dua los yog sib npaug rau | 30 | 25 | 20 | 20 | 15 | 20 | 15 | 15 | |
Cov txheej txheem tsim khoom
1.Raw khoom zoo tswj nrog rau lub cev thiab tshuaj ntsuam xyuas.
2.Crushing thiab sib tsoo ntawm tej raw khoom.
3. Raws li cov neeg siv khoom cov ntaub ntawv yuav tsum tau sib tov Raw Material.
Nias lossis shaping lub cib ntsuab nyob ntawm cov khoom sib txawv thiab cib duab.
4.Dry cov cib ntawm lub tshuab ziab khaub ncaws.
5. Muab cov cib tso rau hauv qhov cub kom kub hnyiab los ntawm qhov kub siab dua ntawm 1300-1800 deg.
6.Lub tuam tsev tswj xyuas qhov zoo yuav tshuaj xyuas qhov ua tiav refractory bricks random.

Packing Thiab Shipping
Ntim raws li kev nyab xeeb hiav txwv-exporting packing Standard
Dispatch: thauj cov khoom tiav ntawm lub Hoobkas los ntawm lub thawv Door toDoor
Los ntawm hiav txwv fumigated ntoo pallet ntxiv cov yas siv ntxiv rau yas zaj duab xis qhwv.

Cim npe nrov: Tuam Tshoj Runner bricks manufacturers, lwm tus neeg, Hoobkas
Tom ntej
Refractory CibKoj Tseem Yuav Zoo Li
Xa kev nug