Corundum Mullite Cib

Corundum Mullite Cib yog ib yam khoom siv refractory uas muaj cov purity alumina. Alumina yog solidified nyob rau hauv lub square thiab tsim low-expansion cib, uas yuav ua rau kom lub kaum sab xis ntub dej ntawm cov kua txheeb ze rau lub refractory theem thiab txhim kho qhov ncaj qha kev sib txuas.
MOQ: 5 tons
Xa kev nug
Khoom Taw qhia
Kev piav qhia

 

Lub corundum mullite cib tau dhau los ua qhov nrov refractory vim nws txoj haujlwm thiab tus nqi sib piv ntawm cov tam sim no muaj qhov kub hnyiab refractories. Vim lawv ntau yam kev sib xyaw thiab kev tsim khoom, ntau hom corundum cib muaj ntau yam kev teeb tsa thiab siv.
Sintered mullite cib thiab fused mullite cib tuaj nyob rau hauv ob hom sib txawv. Moulding thiab hluav taws yog siv los tsim sintered mullite cib, uas feem ntau yog ua los ntawm high-alumina bauxite clinker nrog ib tug me me feem ntawm raw bauxite los yog av nplaum ntxiv raws li ib tug binder.

 

Nta

 

Corundum mullite cib muaj cov thermal conductivity tsawg, muaj zog hanging kiln tawv, siab kub zog, corrosion kuj, thermal shock stability, thiab zoo softening kub nyob rau hauv load.high refractoriness, tsawg kawg yog 1790 degree. Nyob rau hauv load, softening pib ntawm ib tug kub ntawm 1600 thiab 1700 degree. Ntawm qhov kub thiab txias, lub zog compressive yog 70-260 MPa. zoo kam rau ua thermal shock.

 

Daim ntawv thov

 

Kev kub siab ua haujlwm ntawm Corundum mullite cib yog txiav txim siab los ntawm cov ntsiab lus alumina thiab homogeneity ntawm mullite theem thiab iav faib. Feem ntau yog siv rau kub moj tej tawg qhov cub sab saum toj, moj tej tawg rauv ncej thiab hauv qab, iav melting rauv regenerator, ceramic sintering kiln, tuag lub kaum sab xis ntawm roj av cracking system, thiab lwm yam.

 

Physical And Chemical Indicators

 

product-969-373

 

Cov txheej txheem tsim khoom

1.Raw khoom zoo tswj nrog rau lub cev thiab tshuaj ntsuam xyuas.
2.Crushing thiab sib tsoo ntawm tej raw khoom.
3. Raws li cov neeg siv khoom cov ntaub ntawv yuav tsum tau sib tov Raw Material.
Nias lossis shaping lub cib ntsuab nyob ntawm cov khoom sib txawv thiab cib duab.
4.Dry cov cib ntawm lub tshuab ziab khaub ncaws.
5. Muab cov cib tso rau hauv qhov cub kom kub hnyiab los ntawm qhov kub siab dua ntawm 1300-1800 deg.
6.Lub tuam tsev tswj xyuas qhov zoo yuav tshuaj xyuas qhov ua tiav corundum mullite cib random.

product-750-550

Packing Thiab Shipping

 

Ntim raws li kev nyab xeeb hiav txwv-exporting packing Standard
Dispatch: thauj cov khoom tiav ntawm lub Hoobkas los ntawm lub thawv Door toDoor
Los ntawm hiav txwv fumigated ntoo pallet ntxiv cov yas siv ntxiv rau yas zaj duab xis qhwv.

Cim npe nrov: Tuam Tshoj Corundum Mullite Cib, Tuam Tshoj Corundum Mullite Cib manufacturers, lwm tus neeg, Hoobkas

Xa kev nug

whatsapp

Xov tooj

Tug

Kev nug