Ceramic Fiber Board
video

Ceramic Fiber Board

Ceramic fiber board yog ua los ntawm ceramic fiber paj rwb raws li raw khoom, ntxiv ib tug me me ntawm cov organic thiab inorganic binders thiab lwm yam additives, peb muaj ib tug streamlined ntau lawm kab nrog tag nrho automatic tswj thiab advanced technology.
MOQ: 50 daim
Xa kev nug
Khoom Taw qhia
Kev piav qhia

Lub zog ntawm ceramic fiber board yog siab dua li ntawm fiber ntau daim pam thiab lub tshuab nqus tsev tsim cov ntaub ntawv, thiab yog tsim rau high-temperature teb uas yuav tsum tau rigidity thiab lub zog ntawm cov khoom. Qhov saum npoo yog tiaj tus, qhov loj me yog qhov tseeb, qhov toughness yog qhov zoo, nws tuaj yeem txiav ntawm qhov xav tau, thiab cov nyhuv txuag hluav taws xob zoo heev. Nws yog ib yam hauv thiab sab nraud thiab muaj kev ua haujlwm zoo thaum tshav kub kub rwb thaiv tsev.

 

Nta

 

Ceramic fiber board muaj cov yam ntxwv hauv qab no:

1. Zoo heev thermal stability thiab thermal shock kuj

2. Tsawg tshav kub muaj peev xwm

3. Tsawg thermal conductivity

4. Siab compressive zog

5. Zoo toughness

6. Yooj yim rau txheej txheem thiab nruab

 

Daim ntawv thov

 

Ceramic fiber board yog qhov zoo tshaj plaws kev txuag hluav taws xob thiab cov khoom siv hluav taws xob kub rau ntau yam kev lag luam kilns. Nws tuaj yeem siv los ua hauv ob sab phlu, phab ntsa hauv ob sab phlu thiab hauv ob sab phlu rwb thaiv tsev ntawm kilns.

Refractory cib thaub qab ntawm electrolytic txo tank hauv aluminium Hoobkas.

Cov tshuaj tiv thaiv kub siab, phab ntsa hauv ob sab phlu thiab cov khoom siv ntawm cov khoom siv cua sov

 

Physical And Chemical Indicators

 

Khoom & Hom ST BOD GC BOD HA BOD HZ BOD
Specification Kub (degree) 1260 1260 1360 1430
Ua haujlwm kub (degree) 1100 110 1200 1350
Qhov ceev (g / cm3) 280-350 280-350 280-350 280-350
Permanent linear hloov (%) -3
(1000 degree)
-3
(1100 degree)
-3
(1200 degree)
-3
(1350 degree)

 

Thermal conductivity (w / mk)

0.085 (400 degree) 0.085 (400 degree) 0.085 (400 degree) 0.085 (400 degree)
0.132 (800 degree) 0.132 (800 degree) 0.132 (800 degree) 0.132 (800 degree)
0.180 (1000 degree) 0.180 (1000 degree) 0.180 (1000 degree) 0.180 (1000 degree)
Tensile zog (MPa) 0.2 0.2 0.2 0.2

Tshuaj
Kev sib xyaw (%)

Al2O3 38 42 45 39-40
Al2O3 plus SiO2 96 98 99
Al2O3 plus SiO2 plus ZrO2 99
ZrO2 15-17
Fe2O 3 1 0.5 0.5 0.2
Na2O plus K2O 0.5 3 0.2 0.2

 

Cim npe nrov: Tuam Tshoj ceramic fiber board manufacturers, lwm tus neeg, Hoobkas