Soluble Fiber Pam
video

Soluble Fiber Pam

Soluble fiber daim pam, piv nrog cov tsoos inorganic fiber cov ntaub ntawv, cov khoom tsis-fibrous cov ntsiab lus yog txo qis, uas tuaj yeem nce cov ntsiab lus fiber ntau los ntawm 20 feem pua.
MOQ: 50 rolls
Xa kev nug
Khoom Taw qhia
Kev piav qhia

Txoj kab uas hla ntawm cov ntaub soluble fiber ntau yog nyias thiab txhais tes xav tau ntau dua Nws yog mos thiab tuaj yeem txo qhov khaus ntawm daim tawv nqaij ntawm tib neeg thaum siv cov khoom. Vim hais tias nws muaj txaus solubility nyob rau hauv tib neeg lub cev kua ua rau nws nyob rau hauv tib neeg lub cev rau ib tug luv luv lub sij hawm, nws yuav tsis ua kev puas tsuaj rau tib neeg noj qab haus huv, yam tsawg kawg nkaus nws yuav txo tau kev puas tsuaj rau tib neeg noj qab haus huv mus rau qhov tsawg kawg nkaus, yog li nws yog hu ua soluble. fiber ntau. Thiab cov khoom siv fiber ntau yog qhov tsim nyog thiab zoo ib yam, kom ntseeg tau tias cov khoom muaj qis thermal conductivity.

 

Nta

 

Lub thermal conductivity ntawm soluble fiber daim pam yog tsawg, thiab cov khoom ntim me me; Nws muaj qhov zoo ntawm hydrophobicity, lub neej ua haujlwm ntev thiab kev tsim kho yooj yim. Nws tuaj yeem txhim kho qhov kev siv hluav taws xob hluav taws xob zoo, txo cov khoom siv hluav taws xob thiab cov nqi, thiab tsim tus nqi siab dua rau cov neeg siv khoom.

 

Daim ntawv thov

 

Kub rwb thaiv tsev rau steel, petrochemical thiab hluav taws xob fais fab;

Muaj kiln, cua sov ntaus ntawv phab ntsa hauv ob sab phlu, rov qab rwb thaiv tsev;

Cov cuab yeej kub kub thiab cov kav dej rwb thaiv tsev;

Thaum tshav kub kub rwb thaiv tsev thiab tiv thaiv hluav taws ntawm cov khoom siv hluav taws xob;

 

Physical And Chemical Indicators

 

HomCov khoom

Soluble fiber daim pam

Specification Temp. (degree)

1260

Ua haujlwm Temp. (degree)

1100

Qhov ceev (kg / m3)

64

96

128

Linear Shrinkage tom qab cua sov

(%) @ 24 teev

-2.5

(1000 degree)

Tensile zog (MPa)

0.03

0.04

0.05

Fiber ntau (μm)

3.5

Cov ntsiab lus txhaj tshuaj (%)

12

Thermal conductivity (w / mk)

200 degree

0.073

0.065

0.048

400 degree

0.105

0.098

0.087

800 degree

0.176

0.153

0.135

Tshuaj

Kev sib xyaw (%)

SiO 2

55-65 feem pua

CaO

23-35 feem pua

MgO

5-10 feem pua

 

Cov txheej txheem tsim khoom

 

1.Raw khoom zoo tswj nrog rau lub cev thiab tshuaj ntsuam xyuas.

2. crushing thiab sib tsoo ntawm tej raw khoom.

3.Packing tom qab kuaj zoo.

11

 

Packing Thiab Shipping

Ntim raws li kev nyab xeeb hiav txwv-exporting packing Standard
Dispatch: thauj cov khoom tiav ntawm lub Hoobkas los ntawm lub thawv Door toDoor
Los ntawm lub thawv ntawv tawv (Sab nraum) ntxiv rau cov hnab yas (sab hauv).

22

 

Cim npe nrov: Tuam Tshoj soluble fiber ntau daim pam manufacturers, lwm tus neeg, Hoobkas