Daim ntawv Ceramic
video

Daim ntawv Ceramic

Ceramic ntawv feem ntau yog ua los ntawm high purity alumnio-silicate ceramic fiber ntau thiab yog tsim los ntawm cov txheej txheem ntxuav fiber ntau.
MOQ: 50 rolls
Xa kev nug
Khoom Taw qhia
Kev piav qhia

Dab tsi yog ceramic fiber ntawv?

Cov ntawv Ceramic yog ua los ntawm cov purity siab refractory fibers thiab yog npaj rau kub rwb thaiv tsev. Cov txheej txheem tsim khoom siab ua kom muaj qhov sib npaug ntawm cov khoom siv fiber ntau nrog rau kev tswj nruj ntawm cov tuab thiab ntom. Cov ntaub ntawv Ceramic Fiber yog siv los daws ntau yam teeb meem ntsig txog cua sov thiab muaj tshuaj lom neeg ruaj khov, tiv taus cov tshuaj corrosive feem ntau. Ceramic Paper yog cais raws li lawv cov thickness, ntom, fiber ntau index, thiab chemistry. Cov ntawv Ceramic Fiber yog raug rau ntau cov qauv kev lag luam.

 

Nta

Ceramic fiber ntau daim ntawv muaj lub teeb yuag, homogeneous qauv, thiab thermal conductivity tsawg, ua rau nws yog ib qho zoo tagnrho tov rau kub rwb thaiv tsev, tshuaj corrosion kuj, thiab thermal shock kuj. Ceramic Paper muaj ntau yam ntawm refractory thiab sealing siv. Nws muaj cov thermal conductivity tsawg, yoog raws, thiab tuav lub zog zoo.

 

Daim ntawv thov

Ceramic ntawv tuaj yeem siv rau hauv ntau hom kev siv refractory thiab sealing. Xws li kev sib cais lub dav hlau nyob rau hauv lub refractory hauv ob sab phlu, siv nyob rau hauv lub seem seem ntawm cov hlau zawj thiab raws li ib tug kub-sab hauv ob sab phlu. Kev lag luam thiab thaj chaw ua noj ua haus thiab cov khoom siv cua sov rwb thaiv tsev kuj nruab rau nws.

product-300-224

 

Physical And Chemical Indicators

 

Hom 
Cov khoom
DK{0}} DK{0}}350 DK{0}}430
Specification Temp 1000 1100 1300
Kev ceev ceev 200 200 200
Tensile zog 0.4
Cov ntsiab lus organic (%) Tsawg dua los yog sib npaug li 8
Thickness (hli) 0 5-10mm
Dav (mm) 610 hli 1220mm
Tshuaj Kev sib xyaw Al2O3 47 48 40
SiO2 52 51 15-17 ZrO2
Fe2O3 0.5 0.5 0.2
NaO2 0.2  0.2 0.2

 

Cov txheej txheem tsim khoom

Yuav ua li cas yuav ua rau ceramic fiber ntawv?

1. Siv cov tshuaj tsuag fiber ntau (luv fiber ntau, nplua, yooj yim tawg thiab sib xyaw) raws li cov khoom siv raw ntawm ceramic fiber ntawv, ntxiv ib qho kev faib ua feem ntawm cov neeg ua hauj lwm khi thiab cov khoom siv-level additives. Qhov tseem ceeb
2. Siv lub twj tso kua mis nkag mus rau hauv lub pas dej molding thiab do nrog compressed cua. Muab cov pwm tso rau hauv lub pas dej molding thiab siv lub hauv paus ntsiab lus ntawm lub tshuab nqus tsev kom nqus cov fibrous slurry rau pwm. Precisely tswj lub sij hawm adsorption, ua lub tshuab nqus dej ntawm fiber ntau cov ntaub ntawv ntub dej, tshem tawm cov pwm, thiab muab cov neeg rauv qhuav qhuav rau 10-24 teev.
3. Lub tshuab ziab khaub ncaws qhuav yog tswj tau los ntawm lub tshuab tshwj xeeb sib tsoo thiab txiav tshuab kom raug tswj qhov loj.

 

Cim npe nrov: ceramic ntawv, Tuam Tshoj ceramic ntawv manufacturers, lwm tus neeg, Hoobkas