Fireclay Cib
MOQ: 5 tons
Kev piav qhia
Cov txheej txheem ntau lawm ntawm refractory fireclay refractory cib yog muab faib ua raw khoom kho, molding, ziab, kub kub calcination thiab lwm cov kauj ruam. Fireclay cib yog ua los ntawm cov av nplaum hluav taws, calcined chamotte, mullite thiab lwm yam. Cov ntaub ntawv raw ua ntej yuav tsum tau muab sib xyaw rau hauv kev faib ua feem, tshuaj ntsuam thiab hauv av kom tsim tau cov khoom zoo, cov khoom sib xws. Cov cib tsis muaj porosity, siab zog, zoo tiv thaiv thermal spalling thiab abrasion thiab nkag mus. Fireclay refractory cib, tseem hu ua sintered cib, yog ib qho ntawm cov khoom siv tsev qub tshaj plaws hauv ntiaj teb.
Nta
Cov yam ntxwv tshwj xeeb ntawm refractory fireclay cib suav nrog:
Kev kub siab ua haujlwm: Refractory av nplaum cib tuaj yeem tiv taus qhov kub siab txog 2000 degree, yog li lawv tseem tuaj yeem tswj xyuas lub cev thiab tshuaj lom neeg ruaj khov hauv qhov kub thiab txias.
Cov tshuaj tiv thaiv zoo: Refractory av nplaum cib muaj kev tiv thaiv zoo rau cov kua qaub, alkali, ntsev thiab lwm yam tshuaj tiv thaiv corrosion.
Siab zog thiab hardness: Tom qab kub kub calcination, qhov ceev thiab hardness ntawm refractory av nplaum cib yog ho txhim kho, muaj zog thiab hnav tsis kam.
Corrosion tsis kam: Vim tias nws qhov chaw du thiab tiaj tus, nws tsis yooj yim rau nqus plua plav thiab impurities, yog li nws kuj muaj kev tiv thaiv zoo rau cov dej yaig.
Kev ua haujlwm tau zoo: Refractory av nplaum cib tuaj yeem ua tiav ntau yam duab thiab ntau thiab tsawg raws li qhov xav tau ntawm kev siv sib txawv.
Nyob rau hauv luv luv, refractory fireclay cib tau dhau los ua cov khoom siv refractory indispensable nyob rau hauv ntau cov khoom kub kub vim nws zoo heev kub refractory kev ua tau zoo thiab tshuaj stability.
Daim ntawv thov
Fireclay cib yog dav siv nyob rau hauv ob sab phlu coke cub, iav kiln, cement rotary kiln, txiv qaub kiln, txhua yam incinerator, cua sov rauv, thiab lwm yam.
Physical And Chemical Indicators
| Kev piav qhia |
DN -17 |
DN 14 |
DN 12 |
TSI SK34 |
TSI SK33 |
TSI SK32 |
|
| Refractoriness (SK) |
34 |
34 |
34 |
34 |
33 |
32 |
|
| Qhov ceev (g / cm3) |
2.25 |
2.34 |
2.40 |
2.20 |
2.17 |
2.15 |
|
| Txias Crushing Zog (MPa) |
50 |
65 |
70 |
40 |
35 |
30 |
|
| Pom tseeb Porosity (%) |
17 |
14 |
12 |
23 |
24 |
26 |
|
| Kev hloov pauv mus tas li @ 1400ºC * 2hrs (feem pua) |
±0.1~-0.2 |
±0.1~-0.2 |
±0.1~-0.2 |
±0.3 |
±0.5 |
±0.5 |
|
| Thermal Linear expansion @ 1000ºC |
0.6 |
0.6 |
0.5 |
0.6 |
0.6 |
0.6 |
|
| Refractoriness under Load (ºC)@0.2MPa |
1430 |
1470 |
1500 |
1350 |
1300 |
1250 |
|
| Chemical Analysis (%) | Al2O3 |
42 |
45 |
46 |
42 |
38 |
35 |
| Fe2O 3 |
1.7 |
1.5 |
1.3 |
2.0 |
2.2 |
3.0 |
|
Cim npe nrov: Tuam Tshoj fireclay cib manufacturers, lwm tus neeg, Hoobkas