Alumina Ceramic Sab Hauv Phaj Thiab Daim
Khoom Description
Alumina Ceramic Hauv ob sab phlu Phaj Thiab Daim yog ib qho zoo tagnrho cov khoom kub kub refractory nrog zoo heev refractory kev ua tau zoo, hnav tsis kam thiab corrosion kuj, thiab yog dav siv nyob rau hauv high-temperature cov cuab yeej thiab lub cub tawg linings nyob rau hauv metallurgy, iav, tshuaj, hluav taws xob thiab lwm yam lag luam. Nws tuaj yeem tiv thaiv cov cuab yeej los ntawm qhov kub thiab txias thiab corrosion puas, ua kom lub neej kev pab cuam ntawm cov khoom siv, thiab txhim kho kev tsim khoom thiab kev nyab xeeb.
Khoom nta
Hluav taws kub: Alumina muaj qhov kub thiab txias zoo heev thiab tuaj yeem tiv taus qhov kub thiab txias li 1600 degree. Qhov no ua rau alumina ceramic linings yog qhov kev xaiv zoo tshaj plaws rau cov txheej txheem kub xws li metallurgy, iav, tshuaj thiab ceramic industries.
Hnav tsis kam: Alumina Ceramic Hauv ob sab phlu Thiab Daim ntawv muaj kev hnav zoo heev thiab tuaj yeem tiv taus qhov cuam tshuam ntawm kev siv tshuab thiab abrasives. Qhov no ua rau nws dav siv nyob rau hauv ob sab phlu ntawm thee mills, pob mills, mortar mixers thiab lwm yam khoom siv.
Corrosion kuj: Alumina ceramic hauv ob sab phlu muaj tshuaj ruaj khov zoo thiab tuaj yeem tiv taus cov kua qaub thiab alkali daws, corrosive gases thiab molten hlau. Yog li ntawd, nws yog feem ntau siv nyob rau hauv pickling tso tsheb hlau luam, electrolytic tso tsheb hlau luam nyob rau hauv cov tshuaj lom neeg kev lag luam, thiab furnaces thiab ntim nyob rau hauv metallurgy kev lag luam.
Kev ua haujlwm rwb thaiv tsev: Txij li thaum alumina ceramic liners muaj thermal conductivity thiab hluav taws xob tsawg, lawv tuaj yeem muab kev rwb thaiv tsev zoo. Qhov no ua rau lawv siv dav hauv kev lag luam hluav taws xob thiab cov khoom siv hluav taws xob kub kub.
Ntau yam ntawm cov duab: Alumina Ceramic Sab Hauv Phaj Thiab Daim Ntawv tuaj yeem ua rau cov duab sib txawv thiab ntau thiab tsawg raws li kev thov tshwj xeeb. Cov duab uas muaj xws li cib, pobzeb, yeeb nkab, ntoo, thiab cov khoom siv. Qhov kev hloov pauv no tso cai rau alumina ceramic liner hloov mus rau ntau yam khoom siv sib txawv thiab ntau thiab tsawg.

Daim ntawv thov
Kev lag luam metallurgical:Alumina ceramic linings yog dav siv nyob rau hauv ob sab phlu ntawm high-temperature furnaces, smelting furnaces, converters thiab ladles nyob rau hauv lub metallurgical kev lag luam, uas muaj peev xwm tiv taus kub thiab corrosive gases.
Kev lag luam iav:Nws yog dav siv nyob rau hauv cov khoom siv xws li iav furnaces, da dej thiab crucibles nyob rau hauv iav kev lag luam, thiab muaj peev xwm tiv taus qhov tshwj xeeb ib puag ncig ntawm kub kub thiab iav corrosion.
Kev lag luam tshuaj:Alumina Ceramic Liner Plate Thiab Piece feem ntau yog siv rau hauv cov tshuaj tiv thaiv kettles, cov kav dej, cov tso tsheb hlau luam thiab lwm yam khoom siv hauv kev lag luam tshuaj, uas tuaj yeem tiv taus cov kua qaub thiab alkali.
Kev lag luam fais fab:Nws yog siv los ua cov hauv ob sab hauv ntawm boilers thiab cov khoom siv fais fab hauv kev lag luam fais fab, uas tuaj yeem tiv taus qhov kub thiab txias thiab thermal shock.

Kev cog qoob loo
Physical and Chemical Indicators
| Khoom & Hom | 92 Series | 95 Series | 97 Series | 99 Series |
| Qhov ceev (g / cm3) | Ntau dua lossis sib npaug rau 3.63 | Ntau dua lossis sib npaug rau 3.68 | Ntau dua lossis sib npaug rau 3.73 | Ntau dua lossis sib npaug rau 3.83 |
| Moisture Content (%) | Tsawg dua lossis sib npaug rau 0.02 | Tsawg dua lossis sib npaug rau 0.02 | Tsawg dua lossis sib npaug rau 0.02 | Tsawg dua lossis sib npaug rau 0.02 |
| Fracture Toughness (%) | 40 | 42 | 44 | 48 |
| Al2O3 Cov ntsiab lus (%) | Ntau dua lossis sib npaug li 92 | Ntau dua lossis sib npaug li 95 | Ntau dua lossis sib npaug li 97 | Ntau dua lossis sib npaug li 99 |
| Khoov zog | 255 | 275 | 285 | 300 |
Cim npe nrov: Alumina Ceramic hauv ob sab phlu thiab daim, Tuam Tshoj Alumina Ceramic hauv ob sab phlu Phaj Thiab Piece manufacturers, lwm tus neeg, Hoobkas