Ceramic Fiber Ntawv
MOQ: 50 rolls
Kev piav qhia
Ceramic fiber ntau daim ntawv yog ib hom kev sib xyaw insulator tsim los ntawm siab purity ceramic fiber ntau thiab cov ntaub ntawv tshwj xeeb. Nws muaj qhov hluav taws kub zoo heev thiab tuaj yeem tiv taus qhov kub thiab txias tshaj 1300 degree. Nws cov kev tsim tshwj xeeb ua kom ntseeg tau tias nws khaws nws lub zog thiab kev tiv thaiv hluav taws thaum tseem muaj txiaj ntsig zoo txhim kho nws cov cua sov.
Ceramic fiber ntau siv cov khoom siv hluav taws xob zoo rau cov paj rwb, uas dhau los ua cov khoom siv fiber ntau nrog cov purity siab los ntawm crushing, pulping thiab slag tshem tawm cov txheej txheem, thiab diluted nplaum yog ntxiv los ua daim ntawv pulp. Tom qab lub tshuab nqus tsev tsim cov ntaub ntawv ntev ntev, nws yog uniformly qhuav los ntawm microwave, ces dov thiab ntim rau hauv thawv. Nws yog feem ntau siv nyob rau hauv ntau yam xws li tshuaj lom neeg kev lag luam, kev tsim kho kev lag luam, electronics kev lag luam, aerospace kev lag luam, tub rog kev lag luam, cua txias thiab tub yees.
Nta
1. Tsawg thermal conductivity
2. Tsawg cua sov muaj peev xwm
3. thermal shock tsis kam
4. zoo saj zawg zog, tsim kua muag kuj
5. tsis muaj asbestos, tsis ua nrog kua txhuas
6. zoo hluav taws xob rwb thaiv tsev thiab suab rwb thaiv tsev kev ua tau zoo
7. zoo mechanical processing kev ua tau zoo
8. tawv zoo nkauj, siab compressive zog
Daim ntawv thov
Ceramic fiber ntau daim ntawv yog dav siv nyob rau hauv tag nrho cov hom ntawm industrial furnace thiab ladle, lub ladle, submerged nozzle ntawm kub kub rwb thaiv tsev cov ntaub ntawv, muaj hluav taws xob rwb thaiv tsev thiab hluav taws xob rwb thaiv tsev cov ntaub ntawv, lub qhov cub qhov cub thiab lub cub tawg expansion sib koom sealing khoom, txhuas qauv hauv ob sab phlu, microcrystalline iav nrog kub yaj iav daim nyias nyias, kub sealing gasket, cov twj paj nruag thiab cov cuab yeej cua sov ntawm rwb thaiv tsev thiab hluav taws xob insulating cov ntaub ntawv, acoustical rwb thaiv tsev ntawm lub tsheb muffler, lub tso pa yeeb nkab thermal rwb thaiv tsev cov ntaub ntawv, cais ntawm sintering cov ntaub ntawv, warming kuv txhais tes cov khoom muaj nqis rwb thaiv tsev, straightening yob, plaub hau kub rwb thaiv tsev, hluav taws xob thiab hluav taws xob insulating.
Physical And Chemical Indicators
|
Hom Cov khoom |
DK{0}} |
DK{0}} |
DK{0}} |
|
|
Specification Kub (degree) |
1000 |
1100 |
1300 |
|
|
Qhov hnyav (kg / m3) |
200 |
200 |
200 |
|
|
Tensile zog (MPa) |
0.4 |
|||
|
Cov ntsiab lus organic (%) |
Tsawg dua los yog sib npaug li 8 |
|||
|
Thickness (hli) |
0 5-10mm |
|||
|
Dav (mm) |
610 hli 1220mm |
|||
|
ChemicalComposition (%) |
Al2O3 |
47 |
48 |
40 |
|
SiO2 |
52 |
51 |
15-17 ZrO2 |
|
|
Fe2O3 |
0.5 |
0.5 |
0.2 |
|
|
NaO2 |
0.2 |
0.2 |
0.2 |
|
Cov txheej txheem tsim khoom
1.Raw khoom zoo tswj nrog rau lub cev thiab tshuaj ntsuam xyuas.
Muab cov khoom siv raw uas tau xaiv rau hauv qhov cub kom kub kub spinning.
2.Needle nrog lub tshuab koob.
3. Dov li daim pam woven.

Packing Thiab Shipping
Ntim raws li kev nyab xeeb hiav txwv-exporting packing Standard
Dispatch: thauj cov khoom tiav ntawm lub Hoobkas los ntawm lub thawv Door toDoor
Los ntawm lub thawv ntawv tawv (Sab nraum) ntxiv rau cov hnab yas (sab hauv).

Cim npe nrov: Tuam Tshoj ceramic fiber ntau daim ntawv manufacturers, lwm tus neeg, Hoobkas