Honeycomb Ceramic
Khoom Description
Honeycomb ceramic yog tsim los ntawm ntau qhov me me, thiab nws cov qauv zoo ib yam li honeycomb. Nws feem ntau yog tsim los ntawm alumina, silicate, thiab lwm yam additives, thiab ib tug honeycomb-shaped channel qauv yog tsim los ntawm ib tug tshwj xeeb ua txheej txheem. Cov ntaub ntawv no tuaj yeem muab ntau qhov chaw, yog li txhim kho lawv cov haujlwm xws li catalytic cov tshuaj tiv thaiv, pom thiab adsorption. Honeycomb structured ceramics tuaj yeem muab faib ua plaub pawg: khaws cia kub, muab tub lim, catalytic vector thiab lim cov ntaub ntawv. Honeycomb ceramic kub cia kub muaj peev xwm siab tshaj 1000kj / kg, qhov siab tshaj plaws siv kub ntawm cov khoom Ntau dua los yog sib npaug rau 1700 degree C, thiab tuaj yeem txuag tau ntau tshaj 40 feem pua ntawm cov roj hauv qhov cub ntawm qhov cub cua sov, ci, nruab nrab kub cub tawg, thiab tawg cub tawg. Qhov kub ntawm cov roj flue yog tsawg dua 150 ° C.
Nta
Honeycomb ceramic muaj qhov sib piv siab thiab nruj me me pores, thiab muaj lub cev zoo thiab tshuaj lom neeg, xws li lub zog siab, corrosion kuj, kub tsis kam, tsis tshua muaj cua sov coefficient, siab compression zog, thiab lwm yam.

Daim ntawv thov
Hauv cov ntawv thov kev lag luam, cellular ceramics feem ntau yog siv rau hauv tsheb tso pa roj purifiers, cov cuab yeej siv hluav taws xob ua haujlwm, thermal fais fab nroj tsuag thiab cov khoom siv petrochemical. Hauv cov ntawv thov no, honeycomb ceramic tuaj yeem siv los ua tus nqa khoom, siv los kho thiab tawg cov catalyst, thiab tseem tuaj yeem siv los ua lim nruab nrab los txhim kho kev ua haujlwm ntawm cov pa roj. Tsis tas li ntawd, honeycomb structured ceramic kuj tseem siv tau los ua cov khoom siv high-end ceramic xws li lub qhov cub roj, kub-kub sagger, thiab aviation cav nozzle.
Physical and Chemical Indicators
|
Brand Properties |
Honeycomb Cordierite ceramic |
|
Ntev/Dav(MM) |
100 |
|
Ua siab ntev (MM) |
±1.5 |
|
Qhov siab(MM) |
50 |
|
Ua siab ntev (MM) |
±1 |
|
Qhov ceev(Cell/hauv2) |
200 |
|
Nruab nrab phab ntsa tuab(MM) |
0.3 |
|
Ua siab ntev (MM) |
±0.05 |
|
Sab nrauv phab ntsa tuab (MM) |
0.6 |
|
Ua siab ntev (MM) |
±0.2 |
|
Aperture (MM) |
1.8 |
|
Ua siab ntev (MM) |
-0.2 |
|
Kub nthuav dav coefficient(hauv/hauv K) |
1.5- 1.8 |
|
Tshwj xeeb kub muaj peev xwm(J/kgK ib) |
850- 1000 |
|
Khoom siv ceev(kg/m3) |
1800-2000 |
|
Loj ceev(kg/m3) |
500-680 |
|
Nruab nrab hnyav rau ib daim(kg) |
0.3 |
|
Ua siab ntev(kg) |
0.05 |
|
Kub poob siab tsis kam (K) |
Max 500 |
|
Dej nqus (%) |
20-25 |
|
Max ua haujlwm kub (C) |
1300 |
|
Dimension |
Qhov ntau ntawm cov channel |
Phab ntsa tuab |
Sab nraum phab ntsa thickness |
Channel Dav |
Tsis muaj ntu |
Qhov hnyav ib daim |
|
150× 150×300 |
13x13 |
1.5mm ± 0.1 |
1.7mm ± 0.15 |
9. 8- 10mm |
70 feem pua |
3. 8-4.8kg |
|
150× 150×300 |
15x15 |
1.4mm ± 0.1 |
1.6mm ± 0.15 |
8.5 hli |
69 feem pua |
3. 8-4.8kg |
|
150× 150×300 |
25×25 |
1.0mm±{2}}.1 |
1.2mm ± 0.15 |
4. 8-5 0mm |
67 feem pua |
4. 0-5 {2}}kg |
|
150× 150×300 |
32×32 |
{0}.9mm ± 0.1 |
1.2mm ± 0.15 |
3. 8-3.9mm |
61.6 feem pua |
4 6-5.6kg |
|
150× 150×300 |
40×40 |
{{0}}.7mm±0.1 |
1.1mm ± 0.15 |
2 9-3. 1 hli |
64 feem pua |
4 7-5.7kg |
|
150× 150×300 |
43×43 |
{0}}.65mm ± 0.1 |
1.1mm ± 0.15 |
2 7-2.9 hli |
62 feem pua |
4. 8-5.8kg |
|
150× 150×300 |
50×50 |
{0}}.6mm ± 0.1 |
{{0}}.8mm ± 0.15 |
2 3-2.5 hli |
61 feem pua |
4. 8-5.8kg |
|
150× 150×300 |
59×59 |
{0}.45mm ± 0.1 |
{{0}}.8mm ± 0.15 |
1. 9-2. 1 hli |
63.4% ua |
4 7-5.7kg |
Cim npe nrov: Tuam Tshoj Honeycomb Ceramic manufacturers, lwm tus neeg, Hoobkas