May 29, 2024 Tso lus

Yuav ua li cas tshem tawm qhov khoob ntawm Ceramic Fiber Modules?

Ceramic fiber ntau rau hauv ob sab phlu yog maj mam hloov cov tsoos hnyav refractory bricks los ua ib lub ntsiab tshiab rauv hauv ob sab phlu vim lawv qhov zoo ntawm lub teeb yuag, rwb thaiv tsev kub thiab thermal shock resistance. Lub cib pob qij txha ntawm refractory cib rauv linings yog sau nrog refractory av nkos.Ceramic fiber ntau modulesfeem ntau ntsia tau rau hauv ib tug tub rog zoo li kev npaj. Muaj ob hom module qhov khoob, qhov khoob ntawm qhov ntev thiab qhov khoob ntawm qhov dav dav. Yuav ua li cas tshem tawm qhov khoob hauv refractory fiber modules?

 

ceramic fiber modules


1: Kev sib nrig extrusion nyob rau hauv txoj kev dav dav
Ua ntej, lub module dav kev taw qhia muaj compression resilience. Tom qab lub module tau teeb tsa, lub module wrapping daim kab xev raug tshem tawm kom nthuav dav thiab nyem ib leeg, thiab qhov sib txawv ntawm qhov dav ntawm lub module yog txiav tawm.
2: Kev them nyiaj daim pam tshem tawm cov kab sib txawv
Secondly, nyob rau hauv lub ceramic fiber modules ntev kev taw qhia, uas yog, nruab nrab ntawm kab, them nyiaj daim pam yuav tsum tau muab ntxiv kom tau nyiaj them nyob rau hauv lub non-expansion kev taw qhia ntawm lub ceramic fiber module thiab tshem tawm qhov sib txawv ntawm ob kab ntawm modules. Ntawd yog, quav lub daim pam ntawm cov khoom siv tib yam rau hauv U-puab thiab nias nws kom nruj kom sau cov kab sib txawv.
3: Qhov tseeb qhov chaw raws li daim duab kos
Tsis tas li ntawd, qhov tseeb ntawm qhov chaw tseem yog qhov yuav tsum tau ua ua ntej txhawm rau txhim kho kev ncaj ncees ntawm ceramic fiber rauv hauv ob sab phlu. Ua ntej txhim kho lub ceramic fiber module, cov neeg ua haujlwm yuav kos qhov chaw raws li cov duab kos, welding module kho bolts, thiab tsim nyog npaj qhov kev ncua deb ntawm txhua qhov module.
4: Sau nrog ceramic fiber daim pam

Txiav daim pam fiber ntau rau hauv qhov ntau thiab tsawg los sau qhov khoob ntawm cov modules. Txoj kev no yog qhov yooj yim thiab siv tau, thiab tuaj yeem sau qhov khoob zoo thiab txhim kho cov nyhuv rwb thaiv tsev.
5: Sau nrog ceramic fiber ntawv lossis board

Yog tias qhov sib txawv me me, koj tuaj yeem siv cov ntawv fiber ntau ceramic los yog nyias board los sau nws. Txiav nws mus rau hauv ib qho tsim nyog thiab sau rau hauv qhov sib txawv.
6: Ceramic fiber ntau slurry

Siv ceramic fiber slurry los sau qhov sib txawv. Siv ceramic fiber slurry rau qhov sib txawv thiab cia nws qhuav thiab solidify. Txoj kev no yog tsim rau me me thiab tsis sib xws.
7: Stacking installation txoj kev

Thaum txhim kho ceramic fiber modules, siv cov txheej txheem stacking installation. Stagger cov modules kom txo cov tiam ntawm qhov khoob. Txhua txheej ntawm modules yog me ntsis staggered los tsim ib tug ntau-txheej stacking qauv, uas yuav ua tau zoo txo ​​qhov sib txawv.