Jun 03, 2024 Tso lus

Puas Tsawg Cement Castable Yuav Tsum Ntxiv Cov Hlau Fiber Thaum Siv Hauv Cov Sedimentation Chamber?

Yogqis cement castableyog siv nyob rau hauv lub sedimentation chamber, feem ntau, steel fiber tsis tas yuav tsum tau ntxiv.

 

low cement castables


Yog hais tias qhov qis qhib ntawm lub khob hliav qab ntawm cov sedimentation chamber me me dhau lawm thiab yuav tsum tau patted thaum siv, tsuas yog steel fiber ntau yuav tsum tau ntxiv rau cov cement refractory castable uas tsis tshua muaj siv nyob rau hauv lub khob hliav qab kom nce qhov rub, hnav tsis kam thiab yaig. tsis kam. Txawm li cas los xij, yog tias qhov tso tawm ntawm cov sedimentation chamber tsim nyog, thiab qhov loj ntawm cov sedimentation chamber thiab cov rotary kiln kuj tsim nyog, steel fiber tsis tas yuav tsum tau ntxiv rau cov castable.
Qhov kub ntawm cov sedimentation chamber tsis siab, thiab nws tsuas yog ua lub luag haujlwm tshem tawm plua plav. Cov pa roj flue tau poob mus rau hauv qab ua ntej nws ntws tawm ntawm cov sedimentation chamber. Nws yog sau los ntawm cov tshauv hopper nyob rau hauv qab ntawm lub sedimentation chamber, thiab cov unsettled plua plav yog tshem tawm nrog cov flue gas. General low cement castables tuaj yeem ua tau raws li kev siv.
Feem ntau, high-aluminium castables thiab low-cement castables muaj ntau dua, tab sis av nplaum cib kuj tseem siv los ua cov txheej txheem ntawm cov sedimentation chamber, thiab high-aluminium castables kuj siv los ntxiv ib feem ntawm high-voltage hluav taws xob porcelain rau. ua cov castable glaze los pab txhawb kev tsaws ntawm cov pa taws thiab plua plav.
Muaj qee qhov xwm txheej uas cov hlau fiber ntau ntxiv rau cov cement castables tsawg thiab siv rau hauv cov khoom siv sedimentation. Nyob rau hauv xyoo tas los no, cov sedimentation chambers ntawm ib co txiv qaub teb kilns thiab zinc volatilization kilns feem ntau yog lined nrog av nplaum cib. Txawm li cas los xij, qhov loj me tsim ntawm qee cov sedimentation chambers tsis tsim nyog. Thaum cov sedimentation chamber me dhau lawm thiab qhov chaw nres nkoj ntawm lub khob hliav qab kuj me me, cov pa luam yeeb thiab plua plav yuav raug ntaus los daws thaum lub sijhawm tsim khoom. Qhov no yuav ua rau kom lub neej ua haujlwm ntawm cov av nplaum cib lossis cov cement castables qis hauv kab hauv lub khob hliav qab. Yog li ntawd, nyob rau hauv tshwj xeeb, ib tug tsim nyog feem ntawm steel fiber yog ntxiv rau cov uas tsis muaj-cement castable mus ua kom lub hnav tsis kam ntawm lub khob hliav qab seem thiab ua rau nws cov kev pab cuam lub neej.