Precast Block

Precast block tseem hu ua unshaped refractory prefabricated block, yog tsim los ntawm refractory castable thiab refractory plastics.
Xa kev nug
Khoom Taw qhia
Kev piav qhia


Precast block tuaj yeem muab faib ua castPrecast qhob thaiv thiab yas Precast qhob thaiv, muaj aluminate cement, dej iav, Phosphoric acid thiab aluminium phosphate, av nplaum khi thiab qis cement binder prefabricated blocks; Raws li hom aggregate, nws muab faib ua alumina siab, av nplaum, siliceous thiab corundum prefabricated blocks; Raws li txoj kev molding, nws tau muab faib ua kev co molding thiab vibration compression molding Thiab ramming thiab tsim prefabricated blocks; qhov loj ntawm prefabricated blocks yog kaum ob kilograms mus rau ob peb tons, yog li lawv muab faib ua loj, nruab nrab thiab me prefabricated blocks; cov blocks prefabricated yog nruab nrog steel tuav thiab thauj tog rau nkoj, yog li lawv tau muab faib ua cov prefabricated zoo tib yam thiab steel prefabricated blocks. Blocks thiab anchors prefabricated blocks, thiab lwm yam.

 

Nta

1. Nws muaj qhov zoo ntawm qhov kub thiab txias tsis kam, corrosion kuj, abrasion tsis kam, siab zog, thiab zoo thermal shock stability.

2. Kev tsim kho yog yooj yim thiab yooj yim, lub sij hawm tsim kho yog luv, lub sij hawm tsim kho tau txais kev cawmdim, cov nqi tsim kho tau txais kev cawmdim, thiab qhov chaw tsim kho tsis cuam tshuam los ntawm qhov chaw tsim kho thiab cov caij nyoog, ua kom cov kev tsim kho zoo.

3. Tus nqi qis thiab kev nqis peev tsawg

4.Precast blocks yog sib sau ua ke nrog tenon pob qij txha, thiab tsis muaj qhov sib txawv ncaj nraim. Piv nrog rau cov cib refractory, nws tuaj yeem txo cov pob qij txha pob txha pob txha, ua kom lub zog tag nrho ntawm lub tshuab ua kom sov, thiab txo kev siv zog.

 

Daim ntawv thov

Hauv kev lag luam kilns thiab cov khoom siv thermal, Precast qhob blocks yog siv los tsim lub cub tawg, uas tuaj yeem paub txog kev siv tshuab hoisting, txuag kev ua haujlwm thiab kev ua haujlwm, txo lub sijhawm tsim kho, thiab ua kom lub qhov cub ua haujlwm nce.

Precast blocks yuav siv tau los tsim thermal kilns xws li blast furnaces, kub moj tej tawg qhov cub, cua sov rauv, hluav taws xob rauv saum, hlau ore hmoov roasting ncej rauv thiab pellet roasting furnaces. Txog tam sim no, precast blocks tseem siv dav hauv tapping troughs, hluav taws xob rauv saum thiab roasting furnaces. Siv thiab ua lub luag haujlwm ntau dua.

 

Physical And Chemical Indicators

 

Hom /Cov khoom

PCB-RT1

PCB-RT2

PCB-S1

PCB-S2

PCB-D

PCB-W

PCB-WK

Qhov ceev (g / cm3)

2.98

2.85

2.15

2.4

2.43

2.92

3

Txias Crushing zog (MPa)

25

45

30

40

35

28

30

Permanent Linear Hloov @ 1,500 degree x 2H (%)

0.07

-0.09

-0.75

0.5

-0.1

(ntawm 1200 degree)

0.2

-

Chemical Analysis (%)

Al2O3

75

60

45

65

50

90

91

SiO 2

-

-

40

30

-

-

-

MgO

-

-

-

-

-

-

7

Cr2O 3

-

-

-

-

-

7

 

SiC plus C

18

14

8

-

5

-

-

 