Siab zog Castable Refractories
MOQ: 5 tons
Kev piav qhia
Siab zog castables yog tsim los ntawm high-strength aggregates thiab hmoov ntxhia additives. Vim qhov sib ntxiv ntawm high-molecular polymers, lub hauv paus pob zeb yog khov kho.
Nws tuaj yeem siv los ntawm kev ntxiv dej thiab nplawm rau ntawm qhov chaw. Nws muaj kev tsim kho zoo thiab muaj peev xwm ua haujlwm. Ib tug tej thickness ntawm anti-coj txheej yog tsim nyob rau saum npoo ntawm lub silo los yog ore trough los ntawm phau ntawv plastering. Tom qab kev saib xyuas ib txwm muaj, Qhov no refractory castable tuaj yeem ua tau raws li cov kev xav tau thiab muaj kev puas tsuaj. Siab, siab sib txuas lub zog nrog cov pob zeb yooj yim (steel silo), muaj zog cuam tshuam tsis kam, siab compressive zog, zoo durability, ntev kev pab cuam lub neej, thiab lwm yam.
Nta
Lub zog siab castable refractories muaj cov yam ntxwv hauv qab no:
Siab refractoriness
Zoo slag kuj thiab corrosion kuj
Siab zog thiab hnav tsis kam
Zoo thermal shock stability
Zoo kub lub zog
Daim ntawv thov
Lub zog muaj zog castable refractories tshwj xeeb yog siv rau hauv ob sab phlu anti-coj txheej ntawm slag ditch, mine trough, thee discharging trough, hopper thiab cov ntaub ntawv silo hauv metallurgy, thee, thermal zog, tshuaj lom neeg kev lag luam thiab cement industries, thiab rau cov txheej txheem tiv thaiv hnav. ntawm dej nyab sluice thiab unloading hopper nyob rau hauv dej conservancy, hydropower, chaw nres nkoj thiab lwm yam dej num, thiaj li los tiv thaiv lub hauv paus pob zeb.
Physical And Chemical Indicators
|
Hom |
HCA-180 |
HCA-170 |
HCA-160 |
HCA-150 |
HCA-140 |
|
|
Daim ntawv thov txwv Temp degree |
1,800 |
1,700 |
1,600 |
1,500 |
1,400 |
|
|
Qhov ceev (g / cm3) |
2.95 |
2.45 |
2.3 |
2.15 |
2.1 |
|
|
Yuav tsum tau dej rau Casting (%) |
8-11 |
10-14 |
10-14 |
11-15 |
11-15 |
|
|
CCS/MOR (MPa) |
ntawm 110 degree x 24h |
60(10) |
45(8.5) |
40(8) |
40(8) |
35(6) |
|
ntawm 1,200 degree x 3h |
55(9.5) |
50(9) |
45(8.5) |
50(9) |
40(8) |
|
|
ntawm 1,400 degree x 3h |
80(15) |
55(10) |
50(9) |
55(9.5) |
45(8.5) |
|
|
Permanent Linear Hloov (%) |
ntawm 110 degree x 24h |
-0.03 |
-0.06 |
-0.06 |
-0.06 |
-0.06 |
|
ntawm 1,200 degree x 3h |
-0.1 |
-0.2 |
-0.2 |
-0.15 |
-0.15 |
|
|
ntawm 1,400 degree x 3h |
0.4 |
-0.3 |
-0.2 |
-0.3 |
-0.4 |
|
|
Tshuaj ntsuam xyuas (%) |
Al2O3 |
91 |
76 |
63 |
52 |
48 |
|
SiO 2 |
1.5 |
15 |
27 |
40 |
44 |
|
Cim npe nrov: Tuam Tshoj siab zog castable refractories manufacturers, lwm tus neeg, Hoobkas