Bulletproof Alumina Insert Phaj

Bulletproof alumina insert phaj yog nrog cov ntawv zoo Alumina ceramic sab hauv thiab cov xim dub xim dej pov thawj nylon ntaub sab nraud, uas muaj kev tiv thaiv zoo heev thiab nws tuaj yeem ncav cuag qib nij4 tiv thaiv.
MOQ: 5 pcs
Xa kev nug
Khoom Taw qhia
Kev piav qhia

 

Bulletproof alumina insert phaj muaj qhov tshwj xeeb nruj, siab tshwj xeeb lub zog thiab tshuaj inertness hauv ntau qhov chaw. Piv nrog rau cov hlau, Bulletproof Vest Plate yuav plastically deform thiab nqus lub zog thaum tiv thaiv qhov cuam tshuam ntawm cov mos txwv, tab sis nws tsis tshua tsim cov yas deformation, thiab vim nws lub zog siab thiab siab hardness, cov mos txwv tuaj yeem raug passivated lossis txawm tawg, thiab cov ceramic. nto yog crushed nyob rau tib lub sij hawm nyob rau hauv tsim ntawm me me hais. Thiab lub zog tawg ntawm thaj tsam absorbed lub zog ntawm high-ceev warhead.

 

Nta

 

Bulletproof alumina insert phaj muaj cov yam ntxwv ntawm kev ua tau zoo rau tib neeg lub cev nkhaus, siab thiab zoo cov ntsiab lus ntawm raw cov ntaub ntawv, muaj zog tiv thaiv kev ua yeeb yam thiab muaj zog nqus zog.

 

Daim ntawv thov

 

Bulletproof alumina insert phaj yog dav siv nyob rau hauv lub cev armor, tiv thaiv armor rau tsheb thiab aircraft thiab lwm yam khoom siv.

 

Physical And Chemical Indicators

 

Yam khoom Ⅰ Ⅱ
Khoom siv 84.2% Alumina ntxiv rau 14.1% Zirconia 99 feem pua ​​Alumina
Kev tiv thaiv qib NIJⅢ, NIJⅣ NIJⅢ, NIJⅣ
Loj 300 * 250 hli 300 * 250 hli
Khoov zog 457mpa ua 419mpa ua
Elastic Modulus 327 gp ua 315 Gpa ua
Qhov ntom ntom 4.10g / cm33 3.97 g / cm33
Compressive zog Xyoo 1908 Mpa Xyoo 1897 Mpa
Rockwell hardness 90.7 HRA 89.3 HRA

 

Packing Thiab Shipping

 

Ntim raws li kev nyab xeeb hiav txwv-exporting packing Standard
Dispatch: thauj cov khoom tiav ntawm lub Hoobkas los ntawm lub thawv Door toDoor
Los ntawm kev ntim nws nrog ib lub hnab npuas me me thiab muab tso rau hauv lub thawv

 

product-750-521

Cim npe nrov: bulletproof alumina insert phaj, Tuam Tshoj bulletproof alumina insert phaj manufacturers, lwm tus neeg, Hoobkas

Xa kev nug

whatsapp

Xov tooj

Tug

Kev nug