Al2O3-SiC-C cib
video

Al2O3-SiC-C cib

Al2O3-SiC-C cib yog ua los ntawm fused corundum (los yog sintered corundum, tshwj xeeb qib bauxite clinker), graphite thiab silicon carbide nrog taag carbon saum toj no 90%-95% raws li cov ntaub ntawv tseem ceeb.
MOQ: 5 tons
Xa kev nug
Khoom Taw qhia
 
Kev piav qhia

 


Al2O3-SiC-C cib, hu ua ASC cib. Nws yog tsim los ntawm kev ntxiv graphite, bauxite, thiab additives, tom qab batching, sib sau, ziab thiab kub kub tua. ASC cib muaj qhov ua tau zoo ntawm qhov kub thiab txias thiab tiv thaiv oxidation, tiv thaiv flaking thiab anti-slag yaig, tuaj yeem tiv taus qhov kub thiab txias ntawm kev yaig, thiab muaj lub neej ua haujlwm ntev.


Al2O3-SiC-C cib sib xyaw ua kom muaj siab dawb huv alumina (Al2O3), silicon carbide (SiC), thiab carbon (C) ua cov ntaub ntawv tseem ceeb. Alumina ua kom cov refractoriness siab thiab tshuaj stability, thaum silicon carbide txhim khu thermal conductivity thiab abrasion kuj. Cov ntsiab lus carbon optimizes thermal shock kuj thiab corrosion resilience.

 

Al2O3-SiC-C Cib feem ntau yog siv los ua zawv zawg nozzle swb, nruam casting tundish integral stopper, thiab lwm yam. Nws kuj tseem siv tau los ua ob sab rau kub hlau pretreatment thiab steel ladle hauv ob sab phlu. Raws li cov txheej txheem tsim khoom sib txawv, aluminium carbon cib tuaj yeem muab faib ua hluav taws xob aluminium carbon cib thiab tsis siv hluav taws xob aluminium carbon cib.

 

Hluav taws xob aluminium-carbon bricks yog ceramic bonding los yog ceramic-carbon composite bonding khoom. Lawv tau dav siv los ua zawv zawg nozzle slides, ntev nozzles, immersion nozzle sab sauv thiab qis nozzle cib thiab ib qho chaw nres rau nruam casting. Unburned aluminium-carbon bricks yog cov ntaub ntawv carbon-bonded. Vim tias lawv cov oxidation tsis kam yog qhov zoo dua li cov magnesia-carbon bricks thiab corrosion kuj ntawm Na2O slag zoo heev, lawv tau siv dav hauv cov khoom siv hlau kub pretreatment.

 

Nta

 

Exceptional Thermal Stability: Al2O3-SiC-C cib ua rau pom kev ua haujlwm zoo dua thermal, tuav cov txheej txheem kev ncaj ncees ntawm qhov kub thiab txias, dhau ntawm cov khoom siv hluav taws xob.
Txhim kho Mechanical Strength: Kev sib xyaw ua ke ntawm Al2O3, SiC, thiab C muab kev ua haujlwm zoo kawg nkaus, txo qis hnav thiab ua kom muaj kev pabcuam ntev dua hauv qhov chaw hnyav.
Resistance to Thermal Shock: Lub xub ntiag ntawm cov pa roj carbon monoxide ua rau cov thermal shock tsis kam, tseem ceeb heev rau cov kev siv cuam tshuam nrog kev hloov kub ceev.
Zoo heev Corrosion thiab Erosion Resistance: Cov cib no tiv taus corrosive thiab erosive ntsiab, ua rau lawv zoo tagnrho rau kev nruj kev lag luam.
Tsawg porosity: Cov yam ntxwv tsis tshua muaj porosity ua kom cov cua sov tsawg tsawg thiab cov khoom siv rwb thaiv tsev zoo heev.

 

Daim ntawv thov

 

Al2O3-SiC-C Cib yog ib qho ntawm cov khoom siv refractory feem ntau siv rau cov khoom siv thermal siv hauv cov txheej txheem kub kub pretreatment, tshwj xeeb tshaj yog nyob rau hauv cov kub hlau tank, tus nqi siv yog siab heev. Siv dav hauv kev lag luam steel.

 

Physical And Chemical Indicators

 

Al2O3-SiC-C cib
Cov khoom

TC TSI

TSO MZ

TC IB

TSO TR

Pom tseeb Porosity (%)

7

8

8

9

Qhov ceev (g / cm3)

3.00

2.98

2.98

2.93

Txias Crushing Zog (MPa)

55

50

45

45

Thermal Linear Expansion(%) @ 1, 000 degree

0.58

0.55

0.55

0.52

Refractoriness Under Load ( degree )  @0.2MPa

1750

1700

1700

1650

Tshuaj ntsuam xyuas (%)

Al2O3

72

68

67

65

SiC

11

10

10

10

FC

13

12

11

10

Cov ntawv thov tseem ceeb

Torpedo & Hlau Ladle

 

Cov txheej txheem tsim khoom

 

1.Raw khoom zoo tswj nrog rau lub cev thiab tshuaj ntsuam xyuas.
2.Crushing thiab sib tsoo ntawm tej raw khoom.
3. Raws li cov neeg siv khoom cov ntaub ntawv yuav tsum tau sib tov Raw Material.
Nias lossis shaping lub cib ntsuab nyob ntawm cov khoom sib txawv thiab cov cib zoo.
4.Dry cov cib ntawm lub tshuab ziab khaub ncaws.
5. Muab cov cib tso rau hauv qhov cub kom kub hnyiab los ntawm qhov kub siab dua ntawm 1300-1800 deg.
6.Lub tuam tsev tswj xyuas qhov zoo yuav tshuaj xyuas qhov ua tiav refractory bricks random.

 

FAQ

Q: Koj tuaj yeem tswj koj li cas Al2O3-SiC-C cib zoo?

A: TOPOWER muaj ua tiav QC system rau cov tshuaj muaj pes tsawg leeg thiab lub cev muaj zog. Tom qab magnesia ziron bricks ntau lawm, tag nrho cov khoom yuav raug kuaj, thiab daim ntawv pov thawj zoo yuav raug xa nrog cov khoom.

Q: Yuav ntim li cas rau Al2O3-SiC-C cib?

A: Ntim raws li kev nyab xeeb hiav txwv-exporting packing Standard Dispatch: thauj cov khoom tiav ntawm lub Hoobkas los ntawm lub thawv Qhov Rooj ToDoor Los ntawm hiav txwv fumigated ntoo pallet + yas siv + yas zaj duab xis qhwv

 

 

 

 

 

Cim npe nrov: Al2O3-SiC-C cib, Tuam Tshoj Al2O3-SiC-C cib manufacturers, lwm tus neeg, Hoobkas

Xa kev nug

whatsapp

Xov tooj

Tug

Kev nug