Alumina Ceramic Sagger
video

Alumina Ceramic Sagger

Alumina ceramics sagger yog cov khoom siv ceramic nrog a-Al2O3 ua lub ntsiab siv lead ua.Cov ntaub ntawv tseem ceeb ntawm saggers yog cordierite-mullite, mullite, corundum-mullite, alumina, fused quartz lossis cov khoom sib xyaw ntawm cov ntaub ntawv no.
MOQ<5TONS
Xa kev nug
Khoom Taw qhia
Khoom Description

 

Alumina ceramic Saggar yog cov cuab yeej ua khoom noj. Nyob rau hauv tus txheej txheem ntawm firing plooj (porcelain), thiaj li yuav tiv thaiv tau cov roj thiab cov khoom tsis zoo los ntawm kev puas tsuaj thiab defacing lub cev thiab glaze, cov plooj (porcelain) thiab lub cev dawb paug tau muab tso rau hauv cov thawv uas ua los ntawm cov ntaub ntawv refractory rau roasting, uas yog saggar. Nws yog ua los ntawm refractory av nkos ntawm ntau yam specifications ntawm lub round lub tais los yog cuboid, los ntawm kub kub roasting.

 

 

alumina ceramic sagger

 

Khoom nta

 

1. Kev kub siab ua haujlwm: alumina ceramic saggars tuaj yeem tiv taus qhov kub thiab txias yam tsis muaj melting lossis deforming, ua kom ruaj khov ntawm cov khoom ntim khoom thaum lub sijhawm tua hluav taws.
 
2. Chemical inertness: Cov saggars no muaj kev tiv thaiv zoo heev rau cov tshuaj tiv thaiv, kom ntseeg tau tias cov ntaub ntawv raug ua tiav tsis cuam tshuam los ntawm ib puag ncig ib puag ncig.
 
3. Thermal shock resistance: Lawv muaj cov thermal shock tsis kam, tiv thaiv kev tawg lossis kev puas tsuaj thaum raug hloov kub ceev.

 

Cov khoom siv

 

1. Lithium roj teeb: Lithium cobalt oxide, lithium manganese oxide, cobalt oxide, lithium hlau phosphate.

2. Tsis tshua muaj ntiaj teb

3. Sib nqus hlau

4. Mos sib nqus

5. Lub teeb ntes varistor

6. Hluav taws xob ceramics

 

Physical and Chemical Indicators

 

Khoom

Cordierite-Mullite

Mullite-Corundum

Al2O3%

Ntau dua lossis sib npaug li 80

Ntau dua lossis sib npaug li 92

Tsis yog 2%

Tsawg dua los yog sib npaug li 18

Tsawg dua los yog sib npaug li 5

Fe 2O3%

Tsawg dua los yog sib npaug rau 1.2

Tsawg dua lossis sib npaug rau 0.5

Qhov ceev g / Cm3

Ntau dua lossis sib npaug rau 2.6

Ntau dua lossis sib npaug rau 3.7

Thermal Expansion 1000 C

6.5

7.8

Refractoriness C

Ntau dua lossis sib npaug rau 1750

Ntau dua lossis sib npaug rau 1850

Ua haujlwm kub

Tsawg dua lossis sib npaug li 1450

Tsawg dua los yog sib npaug li 1500

 

Cim npe nrov: alumina ceramic sagger, Tuam Tshoj alumina ceramic sagger manufacturers, lwm tus neeg, Hoobkas