Magnesia hercynite cib muab cov txiaj ntsig zoo xws li cov qauv yooj yim dua, chromium-dawb ib puag ncig tiv thaiv, muaj zog thermal shock stability, zoo kiln tawv dai muaj peev xwm, zoo corrosion kuj, thermal expansion, tsis tshua muaj thermal conductivity. Cov tawv nqaij ntawm lub qhov cub tau nrawm nrawm rau hauv qhov chaw tua hluav taws, qhov tuab ntawm daim tawv nqaij yog qhov sib xws thiab ruaj khov, lub cib muaj lub neej kev pab ntau tshaj ib xyoos, tsis muaj qhov tshwm sim loj flaking nrog refractory cib, thiab tsis muaj qhov tshwm sim flaking. refractory bricks thaum lub kiln nres. Qhov kub ntawm qhov cub qhov cub yog qhov tsawg, uas ua rau txo qis hluav taws xob poob.
Nta
Cov yam ntxwv hauv qab no ntawm magnesia hercynite cib:
Zoo heev tiv thaiv corrosion, tsis muaj alkali tawg, loosening, los yog lwm yam teeb meem thaum siv.
Cov tawv nqaij kiln tsim sai, ruaj khov, thiab tsis flake tawm.
Lub siab ntev ntawm cov cement kilns rau qhov kub thiab txias hloov tuaj yeem txhim kho los ntawm kev ua haujlwm zoo thermal poob siab.
Tsis tshua muaj thermal conductivity, lub plhaub rotating kiln nrog qhov kub thiab txias, thiab muaj txiaj ntsig zoo txuag hluav taws xob.
Daim ntawv thov
Magnesia hercynite cib yog dav siv nyob rau hauv ntau yam cement rotary kilns.
Physical And Chemical Indicators
|
Hom /Cov khoom |
MH cib |
|
|
Daim ntawv thov txwv Temp. |
1790 |
|
|
Qhov ceev (g / cm3) |
2.95 |
|
|
Txias Crushing Zog (MPa) |
45 |
|
|
Thermal Shock Resistance ntawm 1,100 degree Dej txias |
6 |
|
|
Refractoriness nyob rau hauv Load (0.2MPa, T2 degree) |
1680 |
|
|
Tshuaj |
MgO |
80 |
|
Kev sib xyaw (%) |
Al2O3 |
4 |
|
Fe2O 3 |
4.0-6.0 |
|
|
Cov ntawv thov tseem ceeb |
- qhov chaw kub hnyiab hauv qhov cub rotary - hloov chaw nyob rau hauv teb kiln |
|
Cov txheej txheem tsim khoom
1.Raw khoom zoo tswj nrog rau lub cev thiab tshuaj ntsuam xyuas.
2.Crushing thiab sib tsoo ntawm tej raw khoom.
3. Raws li cov neeg siv khoom cov ntaub ntawv yuav tsum tau sib tov Raw Material.
Nias lossis shaping lub cib ntsuab nyob ntawm cov khoom sib txawv thiab cib duab.
4.Dry cov cib ntawm lub tshuab ziab khaub ncaws.
5. Muab cov cib tso rau hauv qhov cub kom kub hnyiab los ntawm qhov kub siab dua ntawm 1300-1800 deg.
6.Lub tuam tsev tswj xyuas qhov zoo yuav tshuaj xyuas qhov ua tiav refractory bricks random.

Packing Thiab Shipping
Ntim raws li kev nyab xeeb hiav txwv-exporting packing txuj
Dispatch: xa cov khoom ntim tiav qhov rooj mus rau qhov rooj los ntawm qhov chaw.
Los ntawm hiav txwv fumigated ntoo pallet ntxiv cov yas siv ntxiv rau yas zaj duab xis qhwv.

Cim npe nrov: Tuam Tshoj magnesia hercynite cib, Tuam Tshoj magnesia hercynite cib manufacturers, lwm tus neeg, Hoobkas
Tom ntej
Chrome CibKoj Tseem Yuav Zoo Li
Xa kev nug