Vim li cas thiaj tsis muaj Alumina Cib Siab Siv Ua Hauv Ib Nrab Hauv Alkaline Corrosive Atmosphere?

Cov alkaline, acidic thiab chlorine cov ntsiab lus nyob rau hauv alkaline cua yuav nkag mus tob rau hauv lubsiab alumina cib. Lub neej kev pab cuam luv luv, yog li lub siab alumina hluav taws cib yuav tsum tsis txhob siv los ua cov kab hauv alkaline cua.

 

high alumina bricks

 

1. Alkaline cua yaig yuav ua rau cov kab nrib pleb hauv siab alumina cib

 


Kev yaig ntawm cov huab cua alkaline yuav ua rau ntau qhov kev sib hloov ntawm cov alumina refractory cib siab, thiab xoob ua npuas ncauj yuav tshwm rau ntawm qhov chaw siab ntawm alumina firebricks mus rau thickness ntawm 0-10 hli. Nws tseem yuav ua rau cov cib nthuav dav thiab cov khoom alkaline yuav tsum tau tso rau saum npoo ntawm lub siab alumina hluav taws cib. Sab kub ntawm siab alumina refractory cib, uas yog, siv sab, yuav corroded hnyav dua li sab txias. Yog hais tias qhov chaw siv yog eroded hnyav, lub neej kev pab cuam ntawm lub siab alumina cib yuav luv luv.

 

Ntxiv mus, cov ntsiab lus silica nyob rau hauv siab alumina cib yog siab dua li nyob rau hauv alkaline cib. Qhov siab dua cov ntsiab lus ntawm silicon, qhov ntau dua ntawm cov kua theem tsim, ua rau nws tsis haum rau siv hauv alkaline huab cua hauv ob sab phlu. Cov kua dej ntau dhau deforms cov cib thiab txo lawv lub zog. Lub xub ntiag ntawm dawb silica hauv cib ua rau cov cib muaj kev pheej hmoo ntau dua ntawm kev puas tsuaj.

Thaum cov dawb silica nyob rau hauv lub siab alumina cib tas lawm, lub intrinsic crystalline theem yuav eroded ntau heev. Nyob rau tib lub sijhawm, the thenardite thiab mullite hauv cov cib yuav hnov ​​​​mob ncaj qha rau daim ntawv chert, uas yuav ua rau muaj kev puas tsuaj ntxiv. Siv cov hluav taws kub alumina siab nyob rau hauv alkaline huab cua hauv ob sab phlu tuaj yeem ua rau lub tshuab hluav taws xob hauv ob sab phlu mus sai sai.

 

2. High alumina cib yog cov xov xwm nruab nrab

 


High alumina refractory bricks yog refractory zoo li cov khoom uas yog nruab nrab nruab nrab thiab feem ntau yog siv nyob rau hauv nruab nrab cua. Yog tias siv nyob rau hauv ib qho chaw alkaline, alkali yaig yuav ua rau hauv ob sab phlu ntawm lub cib kom nthuav thiab txo nws lub zog. Thaum ntau qhov ntsuas tau txo qis, qhov kev hloov pauv sab hauv ntawm lub cib yuav tshwm sim. Tom qab kev hloov pauv sab hauv, lub cib hauv ob sab phlu yuav tev tawm lossis txawm tias tev tawm. Qhov no yuav ua rau lub hauv ob sab phlu dheev, ua rau lub qhov cub hauv ob sab phlu tsis tuaj yeem siv tau ib txwm.


Yog li ntawd, tsis txhob siv siab alumina cib rau hauv ob sab phlu hauv alkaline corrosive cua. Kev xaiv ntawm alkaline refractory cib yog ua raws li cov huab cua alkaline, cov huab cua sib koom ua ke, thiab cov alkaline-resistant refractory bricks muaj lub neej ua haujlwm ntev, txo qhov zaus ntawm kev hloov hauv ob sab phlu thiab txo cov peev txheej ntau lawm.

 