Dab tsi ua rau cov kev poob zoo ntawm kev ua kom cov txiv neej refactory casles?

Qhov zoo poob ntawmTsawg Maas Refactory castablestej zaum yuav tshwm sim los ntawm cov laj thawj hauv qab no:

refractory low cement castables


I. Cov Khoom Siv Raw
1 • Cov teeb meem kev kawm kom zoo: Cov ntsiab lus Calcium ntawm cov ntseeg yog qhov tsis ruaj khov, uas yuav tsis muaj zog, lossis kev txhim kho lub zog ntawm cov Castable, ua rau muaj kev poob zoo.
2 • Kev sib sau ua ke thiab cov teeb meem hmoov: tus tsis tsim nyog tau qhab nia sib sau ua ke yuav txo cov kev sib tsoo ntawm cov Castable, thiab txo lub zog. Yog tias cov ncauj lus uas tsis sib haum ntawm cov qoob loo thiab hmoov zoo dua yog tias lawv muaj cov kev ua tau zoo, kev ua kom sov siab ntawm cov metable yuav raug txo kom tsawg.
3 • Cov teeb meem ntxiv rau kev xaiv tsis zoo xws li cov roj av ntxiv xws li flucormal thiab teeb lub sij hawm ntawm cov move refractory caslactory casles.
Ii. Cov txheej txheem ntau lawm
1 • Tsis sib xyaw sib xyaw tsis ncaj: yog lub sijhawm sib xyaw ua ke, xis nyob tsis tau, muaj hmoov sib xyaw ua ke, uas yuav ua tsis tau zoo sib xws, cuam tshuam nrog nws cov kev ua tau zoo.
2 • Lub zog ua kom tsis raug mob hnyav: yog tias lub siab molding siab dhau, lub zog yuav tawg, thiab lub zog ntawm lubast yuav raug txo; Yog tias lub siab yog tsawg dhau, qhov ceev ntawm cov Castable tsis txaus, lub porosity yuav nce ntxiv, thiab lub zog thiab kev tawm tsam erosion yuav raug txo kom tsawg.
3 • Kev Kho Mob Tsis Txaus Siab: Yog tias kev kho qhov kub thiab txias dhau lawm, nws yuav tsis txaus, thiab nws yuav tsis tuaj yeem tau txais lub zog zoo thiab ua tau zoo.
III. Kev tsim kho thiab siv
1 • Teeb meem kev tsim kho ib puag ncig: Yog tias cov kev tsim kho qhov kub tsawg dhau los yog ntau dhau, dej ntawm lubast yuav yaj dhau los lossis qeeb qeeb, cuam tshuam nws cov txheej txheem tawv.
2 • Tsis tsim nyog ci ntsa iab: yog tias cite kub sai sai, cov dej sab hauv kev ntxhov siab ntau, ua rau muaj teeb meem ntau dua, ua kom muaj lwm yam teeb meem, txo nws lub neej pabcuam.
3 • Kev ua haujlwm hnyav hnyav: thaum siv, yog tias nws muaj qhov kub thiab txias, nws yuav ua rau muaj zog ntxiv, nws yuav ua rau muaj kev puas tsuaj rau lub Castable thiab txo nws qhov zoo.