Dab tsi ua rau kev nthuav dav ntawm AZS FUSED BRICKS?

Rau fused cam khwb cia AZS thaiv, yog vim li cas rau qhov nthuav? Tam sim no cia peb saib cov laj thawj rau kev nthuav dav ntawm fused cam khwb cia AZS blocks.

news-300-300

1. Kev nthuav dav ntawm fused cam khwb cia AZS blocks tsis yog nyob ntawm qhov muaj pes tsawg leeg ntawm cov ntaub ntawv raw, tab sis kuj nyob rau ntawm qhov kub thiab txias thiab porosity. Thaum siv nyob rau hauv ib qho chaw ntub dej, rov ua cua sov thiab txias yuav ua rau muaj kev nthuav dav ntxiv, thiab fused cam khwb cia AZS blocks nthuav nrog cov dej kub. nce thiab lub sijhawm ua haujlwm ntev.

2. Txoj kab uas hla ntawm cov dej molecules yog hais txog 0.2um, tab sis cov particles uas tsim fused cam khwb cia AZS block cov ntaub ntawv yog hais txog 1000 npaug loj dua dej molecules, los yog loj dua. Vim lub thermal txav ntawm fused cam khwb cia AZS blocks, dej molecules tuaj yeem nkag mus rau hauv cov khoom yooj yim thiab ua rau tsim cov kab nrib pleb zoo. Tom qab cov pa los yog dej molecules diffused raws phab ntsa microcrack mus txog ib tug nqaim txoj hauj lwm, lub siab ua hauj lwm nyob rau hauv lub sidewall ntawm lub tawg nce mus rau ntau tshaj 100MPa, ua rau cov tawg mus nthuav.

3. Dej vapor yog adsorbed rau ntawm phab ntsa capillary ntawm fused cam khwb cia AZS block; cov ntaub ntawv hydrate los yog slug tov; qee cov ntaub ntawv tsim cov qauv zoo li zeolite; cov iav theem hauv cov khoom yog hydrated; av nplaum ntxhia thiab lawv cov khoom decomposition adsorb noo noo, thiab lwm yam, txhua yam yuav yog vim li cas rau qhov nthuav.

Lub fused cam khwb cia zirconium corundum AZS series khoom tsim los ntawm Topower Refractories yog tsuas yog ua los ntawm industrial alumina, zirconia thiab desiliconized zirconium li raw cov ntaub ntawv. cov khoom tiav.

Topower refractory tsim cov fused cam khwb cia AZS blocks muaj tib co-crystals li AZS33# fused zirconium corundum cib, 36# AZS cib muaj ntau saw-zoo li tus zirconia crystals thiab qis iav theem cov ntsiab lus, yog li corrosion kuj ntawm 36# fused zirconium corundum cib. Cov cuab yeej yog txuas ntxiv txhim kho, yog li nws yog qhov tsim nyog rau thaj chaw uas muaj cov iav nrawm nrawm lossis kub kub.