Cov laj thawj dab tsi rau cov kab nrib pleb hauv Refractory Castable kev tsim kho?

Nrib pleb hauvRefractory CastableKev tsim kho yog feem ntau muaj feem xyuam rau cov khoom zoo, kev sib faib, kev tsim kho tsim kho, txij nkawm thiab siv ib puag ncig.

 

refractory castables


1. Cov teeb meem zoo
a. Tsis txaus cov khoom siv tsis muaj khoom siv purity: yog tias lub raw cov ntaub ntawv raw ntawm casts tsis tau raws cov qauv, lawv yuav muaj ntau impurities. Cov impurities no yuav hnov ​​cov tshuaj ntawm qhov kub thiab txias, ua rau ntim kev hloov pauv, ua rau cov kab nrib pleb. Piv txwv li, cov tshuab hluav taws xob hlau muaj nyob hauv cov khoom nyoos yuav yog oxidized ntawm cov kub, nthuav dav hauv ntim, thiab rhuav tshem cov qauv ntawm cov Castable.
b. Tsis tuaj yeem tsis muaj peev xwm sib cav sib ceg me me: qhov loj me thiab cov qhab nia ntawm cov lus sib sau ua ke yuav cuam tshuam ncaj qha rau kev ua haujlwm ntawm cov Castable. Yog tias cov kev sib sau ua ke loj me me yog qhov nyuaj rau tusyees faib cov txheej txheem loj thaum lub sij hawm vibrating loj thaum lub sijhawm veable, uas tuaj yeem yooj yim rau voids. Thaum cov ntu no tau raug rau kev ntxhov siab los yog kev ntxhov siab txhua yam, cov kab nrib pleb muaj tshwm sim. Ntawm qhov tsis sib xws, yog tias lub aggregate qhov loj me me me me, qhov tshwj xeeb thaj tsam ntawm cov Castable yuav nce, thiab lub zog thiab tawg ntawm cov Castable yuav raug txo.

2. Tsis raug cai
a. Tus nqi tsis raug ntawm phau ntawv: tus binder player playy lub luag haujlwm tseem ceeb hauv Refractory Casab. Nws tuaj yeem ua ke daim ntawv cog lus thiab hmoov ua ke los muab lub Castabet ci ib lub zog thiab lub zog. Yog tias tus nqi ntawm cov phau ntawv me me heev, cov sib khi lub zog ntawm lubast yog tsis txaus ntseeg, thiab cov kab nrib pleb muaj tshwm sim thaum nws raug cov yuam kev sab nraud thaum siv. Ntawm qhov tsis sib xws, yog tias tus nqi ntawm phau ntawv yog ntau dhau, cov dej xav tau ntawm lub Castable yuav nce. Thaum lub sij hawm kho cov txheej txheem, kev hloov dej yuav tawm ntau pores, txo cov ntom ntom thiab lub zog ntawm cov Castable. Nyob rau tib lub sijhawm, cov phau ntawv ntau dhau yuav hloov chaw ntawm qhov kub thiab txias, uas tseem muaj ntau rau cov kab nrib pleb.
b. Tsis tsim nyog siv ntawm Inshixtures: admixtures tuaj yeem txhim kho kev ua tau zoo ntawm refractories casterables. Piv txwv li, cov dej reducers tuaj yeem txo cov dej haus ntawm cov khoom siv casab thiab txhim kho kev nyab xeeb thiab lub zog; Cov neeg sawv cev nthuav tawm tuaj yeem them nyiaj rau lub ntim shrinkage ntawm cov khoom siv ua kom tawv thiab tiv thaiv cov kab nrib pleb. Txawm li cas los xij, yog tias hom admixture tsis yog xaiv los yog cov nyiaj siv tsis tsim nyog, nws yuav tsis tsuas yog ua tsis tiav kev ua tau zoo ntawm cov Castable, tab sis kuj tseem yuav ua rau tawg. Piv txwv li, yog hais tias tus nqi ntawm dej reducer siv yog ntau dhau, lub sij hawm lub sij hawm ntawm lub Castable yuav ntev. Nyob rau lub sijhawm no, cov Castable yog yooj yim cuam tshuam los ntawm lwm cov sab nraud yam thiab cov kab nrib pleb yuav tshwm sim.
3. Kev tsim kho cov txheej txheem txheej txheem
a. Kev sib xyaw tsis ncaj: Refractory Khoom Castables yuav tsum tau do ua ntej kev tsim kho ua ntej kev tsim kho kom ua rau lawv cov yaum kom sib xyaw. Yog tias kev sib xyaw ua ke tsis ncaj, nws yuav ua rau kev faib tawm tsis sib xws ntawm cov khoom siv, thiab cov ntsiab lus ntawm cov chaw hauv zos yuav dhau los lossis tsawg dhau, yog li cuam tshuam kev ua haujlwm ntawm cov Castable. Piv txwv li, yog tias cov ntsiab lus hauv zos siab dhau, cov dej nyob hauv qhov yuav ua rau pom kev ntxhov siab dhau los, ua rau muaj kev ntxhov siab loj, uas yuav ua rau tawg.
b. Uncenpacted kev co: Kev co yog qhov tseem ceeb ntawm cov txheej txheem kev tsim kho ntawm cov khoom siv refractory. Cov kev co tuaj yeem tshem tawm cov huab cua hauv lubast, ua rau nws ntau dua kev cog lus, thiab txhim kho nws lub zog thiab tawg. Yog tias qhov kev vibration tsis tuab, yuav muaj ntau voids thiab npuas nyob sab hauv lubast, thiab cov voids thiab npuas no yuav dhau los ua kev ntxhov siab cov chaw. Thaum cov Castable yog raug rau kev ntxhov siab thermal, kev ntxhov siab txhua yam yog nquag ua kom tawg thiab kev pabcuam lub neej ntawm lub Castable.

4. Tsis Muaj Kev Hlub
a. Kev kho qhov kub yog dhau los yog qis dhau: qhov kev kho kub heev muaj qhov tseem ceeb ntawm kev ua yeeb yam ntawm cov khoom lag luam refractories. Yog tias kev kho qhov kub siab dhau lawm, noo noo hauv lubast yuav yaj nrawm, ua rau muaj kev ntxhov siab sab hauv nruab nrab thiab sab hauv, ua rau tawg. Ib qho ntxiv, kev kho kub heev kuj tseem tuaj yeem ua rau lub zog ua kom tiav thiab ua kom txo qis ntawm cov phau ntawv thiab kev sib sau ua ke, thiab ntxiv mus ntxiv qhov ua tau ntawm cov kab nrib pleb. Ntawm qhov tsis sib xws, yog tias kev kho tus nqi kub dhau lawm, cov txheej txheem hydr Hauv qhov no, cov Castable yog cov yuav ntau dua yuav tawg thaum raug rau sab nraud yuam kev lossis ntsuas kub.
b. Tshuaj Tiv Thaiv Tsis Txaus Ntshai Av noo: Kev kho cov av noo yog ib qho ntawm cov xwm txheej tseem ceeb kom ntseeg tau tias qhov kev coj ua ntawm dej thiab muaj zog ntawm Refractator caster. Yog tias kev kho cov av noo yog qhov tsis txaus, noo noo nyob rau saum npoo ntawm cov av noo, thaum ua kom muaj kev noo noo, thaum sib sau ua kom cov av noo gratity nruab nrab ntawm sab hauv thiab sab hauv. Qhov av noo gratity yuav ua rau kom muaj qhov chaw pov tseg ntau dua li qhov kev nyab xeeb sab hauv, yog li tsim cov tensile ntxhov siab rau saum npoo. Thaum lub tensile ntxhov siab tshaj lub tensile lub zog ntawm lubast, tawg yuav tshwm sim. Tsis tas li ntawd, kev tshuaj ntxuav tsis txaus yuav cuam tshuam txog kev sib txawv ntawm cov kab ke ntawm kev ua haujlwm ntawm cov kas fes, txo qhov kev sib sau ua ke, thiab txuas ntxiv mus tsis muaj zog ntawm cov Castable.
5. Siv teeb meem ib puag ncig
a. Kev hloov pauv kub hloov hluav taws xob kub: Thaum siv cov refrient dab tsi hloov pauv hloov yam, nws yuav ua rau loj thermal kev ntxhov siab hauv lubast. Thaum lub thermal kev ntxhov siab tshaj lub zog txwv ntawm lubast, tawg yuav tshwm sim. Piv txwv li, hauv qee cov tshuaj muaj kuab kilns, nws yog qhov tsim nyog yuav tsum tau pib thiab nres lub cub tawg. Txhua lub sijhawm lub cub tawg tau pib, qhov kub nyob sab hauv lub cub hluav taws xob yuav nce sai. Vim yog lub hysteresis ntawm tshav kub conduction, qhov ntsuas kub ntawm lubast yog tsis sib xws, uas yuav tsim kom muaj kev ntxhov siab rau saum npoo thiab sab hauv. Ntawm qhov tsis sib xws, thaum qhov cub tawg tau nres, qhov kub ntawm cov Castable, thiab kub sab hauv yuav poob qis dua kev ntxhov siab ntawm qhov chaw thiab sab hauv. Txoj kev hloov ntsuas kub no feem ntau yuav ua rau cov kev ntxhov siab hauv lub cev thiab thaum kawg ua rau lub neej tsis tu ncua, cuam tshuam rau cov kev pabcuam lub neej ntawm lub Castable thiab qhov haujlwm ib txwm ua haujlwm ntawm cov kiln.
b. Tshuaj Yis Yis Yis Yis Yis Yis: Hauv qee qhov kev siv ib puag ncig, Refractory castables yuav yaig los ntawm cov tshuaj yeeb, ua rau cov kab nrib pleb. Piv txwv li, nyob rau qee cov kilns hauv metallurgy, xws li cov roj dulfur, thiab cov soclefur trioxide, thiab so kua txiv hydrochoxide, thiab lwm yam). Cov tshuaj no yuav hnov ​​cov tshuaj uas muaj qee cov khoom siv hauv cov Castable los tsim cov teb tshiab. Cov kev tsim kho no tshiab tau muaj cov khoom sib txawv thiab cov khoom sib txawv, uas yuav ua rau muaj kev ntxhov siab hauv lub Castable. Thaum qhov kev ntxhov siab no tshaj li lub zog txwv ntawm lubast, kev tawg yuav tshwm sim. Ib qho ntxiv, tshuaj yaig kuj tseem tuaj yeem rhuav tshem cov qauv ntawm cov Castable, txo qhov kev ua haujlwm ntawm lub Castable, thiab cuam tshuam txog kev ua haujlwm ib txwm muaj ntawm cov kiln.