Nyob rau hauv tsab xov xwm kawg, qhov tseem ceeb ua ke ntawm cov ntaub ntawv refractory yog tham txog. Cia peb saib ntawm qhov sib xyaw ua ke ntawm cov hluav taws kub nyhiab thiab cov khoom siv refractory.
Cov ntaub ntawv refractory feem ntau yog Tuam Tshoj Refractory Brick, siab aluminium cib, castable, siab aluminium refractory cib, thermal rwb thaiv tsev cib, siab aluminium hnav-resistant cib, av nplaum thermal rwb thaiv tsev cib, lub teeb siab aluminium cib. Kev sib xyaw ua ke ntawm cov khoom siv refractory hauv cov txheej txheem ntawm kev siv muaj rau hauv qab no rau:
(1) Kev sib xyaw ua kua dej - los ntawm kev siv cov tshuaj tiv thaiv hydration ntawm tus neeg sawv cev platform thiab dej ntawm chav tsev kub los tsim cov khoom hydration, kev sib xyaw ua ke tshwm sim.
(2) Chemical binding - Kev sib khi tshwm sim los ntawm kev siv tshuaj lom neeg ntawm cov ntawv khi thiab cov tawv tawv, los yog cov ntaub ntawv thiab cov khoom siv refractory nyob rau hauv chav tsev kub, los yog cov tshuaj tiv thaiv thaum lub sij hawm cua sov los tsim cov tebchaw uas ua raws li binders.
(3) Polymerization binding - los ntawm kev ntxiv cov catalyst lossis crosslinking tus neeg sawv cev, lub zog khi yog tsim los ntawm kev sib xyaw ua ke polymerization ntawm tus neeg sawv cev khi los tsim cov qauv sib txuas.
(4) Ceramic ua ke - hais txog qhov kub thiab txias sintering ua ke, uas yog, ntxiv additives los yog hlau hmoov nyob rau hauv tej refractory yuav txo tau lub sintering kub, thiaj li yuav txo tau cov kua theem kub, txhawb cov khoom-kua cov tshuaj tiv thaiv ntawm tsawg kub. thiab ua kom tsis tshua muaj kub sintering ua ke.
(5) Adhesion binding - yog tsim los ntawm ib qho ntawm cov kev ua hauv qab no.
1. Lub cev adsorption: nyob ntawm kev sib cuam tshuam ntawm molecules ib van der Waals quab yuam thiab kev sib xyaw ua ke ntawm;
2. Diffusion nyhuv: nyob rau hauv qhov kev txiav txim ntawm lub thermal txav ntawm cov khoom molecules, cov binder thiab cov molecules ntawm cov nplaum muaj kev sib nrig sib diffusion nyhuv, tsim ib tug diffusion txheej, thiaj li mus tsim ib tug ruaj khov ua ke;
3. Electrostatic nkaus: muaj ob txheej hluav taws xob ntawm qhov sib cuam tshuam ntawm cov ntawv khi thiab cov nplaum, uas yog ua ke los ntawm electrostatic attraction ntawm ob txheej hluav taws xob.
(6) Condensation thiab binding - lub condensation ntawm microparticles (colloidal hais) los ntawm kev ntxiv ib tug condensate tus neeg sawv cev rau kev khi.
Topower refractory li Tuam Tshoj Refractory Cib suppiler tuaj yeem muab qee qhov zoo Tuam Tshoj Refractory Bricks, insualtion thremal cov ntaub ntawv, refractory raw khoom thiab ntau yam refractory hluav taws cib. Peb lub tuam txhab muaj cov kws tshaj lij pab pawg, txhua yam khoom raug soj ntsuam nruj me ntsis, kom ntseeg tau tias cov neeg siv khoom yuav cov khoom zoo, muab kev pabcuam huab cua tom qab muag tag nrho, yog tias koj muaj teeb meem nrog cov khoom, koj tuaj yeem tiv tauj peb txhua lub sijhawm. .