Cov kev sib txuas ua ke ntawm cov khib nyiab roj hluav taws xob yog ib txheej ntawm cov khoom siv refractory rau cov ntaub ntawv ntawm cov tshuab cua sov. Hom kev pov tseg roj tsis sib xws yog tsis zoo li smelting rauv hauv kev lag luam steel, uas muaj kev kub ntxhov thiab hnav lub cev puas tsuaj. Cov xwm txheej uas muaj kev cuam tshuam ntawm cov khib nyiab roj hluav taws xob hluav taws xob tsis tau muab faib ua peb theem: preheating thiab txias.

Cov qauv kev xaiv tsim nyog ntawm tus qauv rau lub zog tsis tuaj yeem tiv thaiv cov txiaj ntsig zoo thermal thiab txuas ntxiv lub neej ua haujlwm ntawm lub cub hluav taws. Tam sim no, muaj ob hom kev loj rau cov hluav taws xob: ib qho yog refractory cib, Refractory Castables; Haum rau kev sib txuas ua si ntau dua 1200 degree, thiab lwm yam yog qhov tsawg-kub 900 degree incineration ib puag ncig uas tau siv tag nrhoTej hub Fiber ModuleTus qauv pob.
Raws li lub teeb yuag thiab txuag hluav taws xob zoo li qub, cov kev ua tau zoo sib xyaw muaj cov kev ua tiav hauv qab no piv nrog cov roj hmab refractory:
(1) Cov tuab ntom ntom ntom ntom ntom. Tus Ceramic Fiber Folding Module Rwb Thaiv Tsev Loj, uas tuaj yeem txo cov qauv ntawm lub neej ntawm lub neej ntawm cov cua cub.
(2) Tsawg thermal muaj peev xwm. Lub peev xwm thermal ntawm ceramic fiber yog tsuas yog 1/7 ntawm lub teeb ci kub-resistant cov pob zeb hauv hluav taws xob, tshwj xeeb tshaj yog rau cov cua sov kev siv hluav taws xob.
(3) tsis muaj thermal conductivity. Lub thermal conductivity ntawm tus ceramic fiber module yog tsawg dua {2 {{{{{{{{{{{{{{{{{{{{{{ kub-resistant casableable.
(4) Cov cua sov zoo heev tiv thaiv thiab tshuab kev co tshuab. Ceramic Fiber Foldable Modules yog hloov tau thiab muaj kev tiv thaiv zoo heev rau qhov kub thiab cua hloov khoom siv thiab tshuab deeg.
(5) kev tsim kho yooj yim. Anchor ntsia hlau yog yooj yim rau weld, thiab lawv cov tshwj xeeb anchoring txoj kev daws cov teeb meem ntawm kev teeb tsa qeeb ntawm cov npo qeeb. Tom qab cov modules folding yog untied, lawv yuav nyem txhua lwm yam hauv cov lus sib txawv tsis muaj cov khoom sib txawv. Lub cub hluavtaws tsis tas yuav qhuav lossis tswj thiab tuaj yeem siv ncaj qha tom qab kev teeb tsa.
Qhov tsis zoo ntawm Ceramic Fiber Modules tau siv nyob rau hauv incinerators yog tias qhov siab tshaj plaws los ua kom muaj roj ntau dua nrog kev nce siab ntawm kev ua haujlwm kub. Txhuam hniav lossis txau cov txheej saum npoo av ntawm cov ceramic fiber folding mold scouring thiab flue roj intrusion ntawm cov rauv fiber ntau hauv cov kab mob fiber ntau. Txawm li cas los xij, txij li qhov kev txiav tawm ntawm qee qhov chaw kub ntawm cov khoom kub uas muaj qhov tsis sib xws nrog tus qauv, cov txheej ntau feem ntau tawg thaum lub sijhawm ua haujlwm. Yog li ntawd, nws raug nquahu kom tsis txhob siv cov txheej txheem sib tw saum npoo av kom txhim kho cov pa hluav taws yaig tawm tsam fiber ntau. Yog tias tsim nyog, ib qho kev sib txuam saum npoo av yuav tsum tau siv los txhim kho cov pa hluav taws yaig tawm tsam ntawm cov fiber module hauv ob sab.