Lub zog hluav taws xob rwb thaiv tsev stainless hlaurefractory thauj tog rau nkojKev muag khoom, Cov neeg siv khoom hauv Kaus Lim Kauslim xaj 20 Tons

Refractory Anchors yog cov pob txha pob txha uas txhawb nqa cov khoom siv hluav taws xob los yog cov khoom siv refractory prefabricated los txhim kho cov refractory hauv ob sab phlu kom tiv taus cov khoom zoo li qub, thermal stress, mechanical expansion thiab mechanical vibration. Cov teeb meem dab tsi ntawm cov thauj tog rau nkoj yuav cuam tshuam ncaj qha rau kev pabcuam lub neej thiab kev nyab xeeb ntawm cov khoom siv refractory?
01 Dimensional deviation ntawm thauj tog rau nkoj manufacturing
Feem ntau, cov thauj tog rau nkoj yog tsim nyob rau hauv ntau qhov ntau, tab sis cov cuab yeej ua haujlwm yog qhov yooj yim thiab kev tswj tsis tau paub txog nws, uas ua rau cov khoom qis qis, txoj kab uas hla me me thiab nyias nyias. Cov khoom siv kho tshuab ntawm cov khoom zoo li no yog qhov tsawg. Thaum xaj, cov tuam txhab cement feem ntau tsuas yog xav tau qhov loj thiab qhov hnyav. Nws raug pom zoo tias cov tuam txhab xa mus rau txoj kab uas hla tus qauv kev cai ntawm puag ncig steel hauv kev lees paub ntawm anchors. Thaum lub chaw tsim khoom thauj tog rau nkoj pub cov khoom siv, qhov loj ntawm cov khoom yuav tsum tau tswj nruj me ntsis thiab cov txheej txheem tshuaj xyuas thiab cov txheej txheem yuav tsum tau ua. Thaum lub tuam txhab lees txais ca steel anchors, qhov sib txawv ntawm cov khoom thickness thiab dav yuav tsum tau kuaj xyuas. Thaum txais cov khoom siv thiab cov khoom tiav, vernier calipers thiab steel kav feem ntau yog siv los xyuas cov kab thiab qhov ntev.
02 Manufacturing shape of anchors
Ib qho teeb meem hauv kev tsim kho kiln hauv ob sab phlu yog tias cov qauv ntawm cov anchors tsis yog raws li tus qauv. Cov kev xav tau xoob ntawm cov duab geometric thiab curvatures ntawm cov thauj tog rau nkoj yuav pab txhawb kev tsim khoom thiab kev tsim khoom, tab sis yuav ua rau poob nyiaj txiag rau cov kab ntau lawm. Cov cuab yeej siv cua sov castables thiab refractory anchors yuav muaj kev ntxhov siab tso tawm, nthuav dav thiab kev cog lus thaum kub kub thiab kub hloov pauv thaum ua haujlwm. Yog hais tias lub kaum sab xis geometric thiab curvature ntawm cov anchors muaj qhov sib txawv loj, lawv cov kev ntxhov siab tso tawm, nthuav dav thiab kev cog lus yuav txawv. Qhov sib txawv no yuav ua rau cov kab nrib pleb hauv cov castable refractory, looseness thiab detachment ntxov ntxov, thiab nws thiaj li ua rau lub plhaub liab tshwm sim ntawm cov khoom siv thermal. Yog li ntawd, cov kev cai nruj ntawm kev tsim cov duab ntawm cov thauj tog rau nkoj yog ib qho teeb meem loj ntsig txog kev pab cuam lub neej ntawm refractory castables.
03 Cov khoom ntawm anchors
Hauv kev sim cov khoom siv ntawm cov thauj tog rau nkoj, peb feem ntau pom tias cov ntsiab lus ntawm Ni thiab Cr yog qhov tsawg, thiab tseem muaj kev faib tawm tsis sib xws ntawm cov ntsiab lus ntawm cov khoom siv, uas yuav cuam tshuam rau cov khoom siv hluav taws xob thiab cov cua sov ntawm cov khoom, yog li txo cov khoom siv. kev pab lub neej ntawm cov castables tuav. Cov cuab yeej tshuaj xyuas rau cov khoom thauj tog rau nkoj feem ntau yog siv cov khoom siv tes los yog cov duab spectrometers, thiab qhov kev tshuaj xyuas ntau thiab qhov tseeb yog txawv me ntsis. Ua ntej kev soj ntsuam, cov qauv ntsuas ntsuas yuav tsum tau siv los txheeb xyuas qhov tseeb ntawm cov cuab yeej ntsuas thiab xyuas qhov tseeb.
04 Vuam ntawm thauj tog rau nkoj manufacturing
Ib qho ntawm cov yam ntxwv cuam tshuam rau qhov zoo ntawm cov khoom siv hauv tsev yog qhov refractory thauj tog rau nkoj vuam tsis yog raws li tus qauv. Cov qauv ntawm cov thauj tog rau nkoj yog qhov yooj yim, thiab cov kev xav tau vuam feem ntau tsis quav ntsej hauv kev tsim khoom. Tsis quav ntsej cov kev cai vuam yog qhov tseem ceeb tsis quav ntsej lub luag haujlwm ntawm cov qauv thauj tog rau nkoj, uas yuav ua rau lub thauj tog rau nkoj bearing muaj peev xwm tsawg thiab tsis tuaj yeem tiv taus cov kev hloov pauv hauv qhov hnyav thiab cov cua sov. Yog li ntawd, thaum welding anchors, ntawm ib sab tes, kev xaiv cov khoom siv vuam yuav tsum ua raws li cov txheej txheem vuam ntawm cov ntaub ntawv, thiab ntawm qhov tod tes, nws yog ib qho tsim nyog los tiv thaiv spatter, vuam slag, tawg, undercuts, thiab txheej tu.
05 Tsim cov duab kos thiab specifications ntawm anchors
Cov qauv kos duab thiab cov lus qhia tshwj xeeb ntawm cov thauj tog rau nkoj tsis sib koom ua ke, thiab cov chaw tsim khoom yuav xav tias cov khoom lag luam yog qhov tsis txaus ntseeg, yog li cov txheej txheem ua thiab xaiv cov khoom siv kuj yog arbitrary, thiab qhov tseeb qhov tseeb kuj txawv. Cov ntaub ntawv muaj xws li kos duab txias, kub dov, ci round steel, thiab dub round steel. Cov qauv kos duab ntawm cov thauj tog rau nkoj feem ntau yog pub dawb. Txij li thaum qhov ntau ntawm kev zam pub dawb yog qhov loj, kev nkag siab ntawm cov tuam ntxhab kuj tsis sib xws, thiab qhov ntau thiab tsawg ntawm cov khoom tsim tawm yuav txawv. Yog li ntawd, nws raug pom zoo tias thaum tsim cov thauj tog rau nkoj, qhov loj me yuav tsum muaj kev sib koom ua ke thiab meej, uas tsis tsuas yog yooj yim rau cov neeg tsim khoom kom muaj cov kev xav tau los siv, tab sis kuj yooj yim rau cov neeg soj ntsuam zoo kom muaj lub hauv paus meej los xyuas qhov tseeb ntawm txhua qhov. ib feem. Kev zam pub dawb tuaj yeem xa mus rau cov kev cai cuam tshuam ntawm GB/T1804-1992 "Unmarked Tolerances of Linear Dimensions".
06 Sampling inspection method for anchor quality soj ntsuam
Cov qauv tshuaj ntsuam xyuas txoj hauv kev rau kev kuaj xyuas cov khoom siv hluav taws xob zoo yuav tsum yog ob qho tib si zoo thiab kev tshawb fawb. Rau qee qhov ntau yam nrog ntau qhov ntau, kev tshuaj xyuas cov qauv tuaj yeem ua tiav los ntawm kev xav ua piv txwv, random sampling, stratified random sampling, thawj sampling, thib ob sampling thiab lwm txoj kev, thiab txhua hom yuav tsum tau soj ntsuam ntau li ntau tau. Tus lej loj ntawm cov qauv yuav tsum muaj ntau dua los ua kom cov neeg sawv cev ntawm batch sampling. Cov txheej txheem tshuaj xyuas zoo rau cov thauj tog rau nkoj yog: cov khoom siv ntawm cov thauj tog rau nkoj → zoo li → txoj kab uas hla lossis thickness, ntev, kaum sab xis, curvature, thiab lwm yam.; kev tsom xam ntawm cov thauj tog rau nkoj yuav tsum khaws cov ntaub ntawv pov thawj spectral tsom xam kom yooj yim traceability thaum siv yav tom ntej; Nyob rau tib lub sijhawm, nws yuav tsum muab cov ntaub ntawv zoo xws li daim ntawv pov thawj Hoobkas ntawm cov khoom siv raw ntawm cov thauj tog rau nkoj sib xws thiab cov ntawv xeem muaj pes tsawg leeg; Kev kuaj xyuas qhov chaw thiab cov qauv ntsuas thiab cov kev xav tau rau cov thauj tog rau nkoj yuav tsum ua kom tiav raws li qhov ua tau, uas yog, cov qauv yuav tsum tau khaws cia rau txhua yam khoom, thiab cov qauv yuav tsum tau khaws cia rau cov khoom loj, thiab qhov kev siv thiab cov qauv ntawm cov qauv yuav tsum tau nce kom tsim nyog.