Cov ntsiab cai thiab cov kev ceev faj rau kho cov cib rectractory hauv kev lag luam KILNs

Refractor Cibyog cov ntaub ntawv tseem ceeb rau cov khoom siv hauv cov khoom siv. Lawv feem ntau muaj kev sib tua hluav taws kub. Tsim nyog cov neeg rectractories feem ntau yog siv rau lub sijhawm ntev ntawm cov khoom muaj peev xwm. Txawm li cas los xij, vim muaj kev cuam tshuam ntawm cov xwm txheej sab nraud, qee cov kab mob hluav taws yuav yog ib nrab puas. Hauv qhov no, peb yuav tsum tswj thiab kho cov cib no. Feem ntau, peb paub tias refractory firmicks tsim los ntawm kev muaj kev lag luam kilds ntawm kev kho ntawm magnesia {{chrome cib thiab spinel cib.

high alumina refractory brick


Cov hauv qab no yuav qhia rau koj cov teeb meem uas yuav tsum tau them nyiaj rau thaum kho cov cib:
1. Cov cib siv rau lub patching yuav tsum yog los ntawm cov chaw tsim khoom tib yam thiab tib lub pob ua cov thwv cib qub;

2. Siv cov cib ntxiv los ntawm kev saib xyuas tib yam li cov pob zeb qub kom ntau li ntau tau (CEEB TOOM: Cib uas tsis tshua muaj kev txwv tsis pub);

3. Tus neeg sib tiv tauj ntawm cov thwv cib tshiab thiab qub yuav tsum colled;

4. Tsis muaj hlau phaj tuaj yeem muab tso rau ntawm cov chaw sib cuam tshuam ntawm qhov tshiab thiab qub refractory cib;

5. Tsis muaj cov hlau hlau tuaj yeem muab tso rau ntawm cov leeg khi cib ntawm ob sab ntawm lub xauv cib. Cov hlau hlau ntawm ob lub rooj sib txuas uas nyob ib sab ntawm cov cib yuav tsum yog staggered, thiab tsis muaj hlau ntim tau muab tso rau ob sab ntawm tib lub cib;

6. Cov hlau phaj yuav tsum raug muab tso rau hauv cov nqaj qaum;

7.

8. Masonry yuav tsum tau nqa tawm nruj me ntsis raws li cov tsim cib piv, thiab masonry piv yuav tsum tsis txhob hloov pauv ntawm yuav;

9. Cov ntawv nthuav dav sib txuas ntawm cov pob zeb ua kom ntub dej yuav tsum tsis txhob ntub dej ntawm lub taub hau loj.

10. Sim tsis txhob siv (lossis txo cov siv ntawm) cov cib ua thaum patching.
Cov hauv paus ntsiab lus ntawm kev thaj chaw refractory
Cib yuav tsum tau qhib los ntawm qhov tsis muaj zog tshaj plaws ntawm lub cib, tab sis tsis muaj ntau tshaj peb lub nplhaib ntawm cov cib tuaj yeem khawb tau tib lub sijhawm. Yog tias nws yog ib qho kev nruam ntau- Nplhaib ua kom tiv thaiv lub cib, kom muaj kev txo qis, nws yog ib qho tsim nyog yuav tsum tau thaj 2 cov nplhaib ua ntej txuas ntxiv mus rau sab rov qab. Thaum khawb cov cib, ua tib zoo mloog kom nruj ntawm cov cib tag nrho. Yog tias cov cib yog xoob xoob tas nrho, nres khawb tam sim ntawd, thiab siv pob zeb xov tooj hlau khi ntawm ob sab ntawm cov cib xoob. Tom qab zawm, paub meej tias lawv tsis plam ua ntej txuas ntxiv ua haujlwm.