Jul 27, 2023 Tso lus

Hluav Taws Cib Kev Muag Khoom, Cov Neeg Siv Khoom hauv Switzerland Ordered 53 Tons

Thaum Lub Xya Hli 53 tons Hluav Taws cib tau ntim rau kev xa mus rau cov neeg siv khoom hauv Switzerland. Zoo siab thiab zoo tus nqi refractory cib hauv Topower Refractory.

 

Tam sim no, firebrick yog ib qho ntawm feem ntau cib siv nyob rau hauv kev tsim kho kev lag luam. Koj puas paub qhov specifications thiab qhov ntau thiab tsawg nws muaj?

 

Hluav taws kubyog ib hom kev kub siab resistant lub tsev khoom, uas yog tsim los ntawm av nplaum, txhuas hmoov, calcium hmoov thiab quartz xuab zeb. Vim nws cov hluav taws kub zoo heev, tiv thaiv corrosion, tsis tshua muaj cua sov thiab lwm yam zoo, nws yog dav siv nyob rau hauv thermal khoom nyob rau hauv ib qho tseem ceeb industrial qhov chaw, xws li thermal fais fab chaw nres tsheb, boilers thiab automotive internal combustion xyaw, alkali, nitrate thiab ore cov ntaub ntawv. Refractory cib muaj lub zog siab, zoo thermal shock kuj thiab khoov lub zog, yog li nws muaj lub neej ua haujlwm ntev. Tsis tas li ntawd, nws muaj ntau qhov sib txawv thiab qhov ntau thiab tsawg, yog li nws muaj ntau yam kev siv. Raws li nws cov duab thiab qhov loj tuaj yeem muab faib ua cov cib zoo tib yam, cov qauv cib, cov cib tshwj xeeb thiab lwm yam.

 

Refractory cib muaj lub zog siab, zoo thermal shock kuj thiab khoov lub zog, yog li nws muaj lub neej ua haujlwm ntev. Tsis tas li ntawd, nws muaj ntau qhov sib txawv thiab qhov ntau thiab tsawg, yog li nws muaj ntau yam kev siv. Raws li nws cov duab thiab qhov loj tuaj yeem muab faib ua cov cib zoo tib yam, cov qauv cib, cov cib tshwj xeeb thiab lwm yam.

 

firebrick

 

1. Ordinary firebrick: tiav chav ntsuas qhov hnyav 2-8 kg, tsis pub ntau tshaj 4 ntsuas ntsuas, qhia qhov loj me piv rau hauv thaj tsam ntawm 1: 4, tsis muaj concave fab, qhov, grooves.

2. Txheem cib specification loj: Cov qauv cib yog T-3 refractory cib, qhov ntev yog 230 * 113 * 65, 23011365-55, 25012365, 25012365-55 (mm). T-1:172*114*65, T-2:230*114*32.

3. Zoo li firebrick: unit hnyav 2-15kg, tag nrho qhov loj piv yog tsawg dua 1:6, thiab lub concave lub kaum sab xis tsis ntau tshaj ob; Los yog muaj lub kaum sab xis ntawm 50-75 degrees; Los yog cov khoom uas tsis muaj ntau tshaj plaub grooves.

4. Cov cib tshwj xeeb: qhov twg qhov hnyav ntawm cov khoom tiav yog nyob nruab nrab ntawm 1.5-30 kg.

Cov saum toj no yog lub ntsiab specifications thiab qhov ntau thiab tsawg ntawm firebricks, thiab cov khoom ntawm txawv specifications thiab ntau thiab tsawg yuav ua tau raws li cov kev xav tau ntawm cov neeg muas zaub nyob rau hauv txawv zaus. Yog tias cov neeg siv khoom muaj kev xav tau tshwj xeeb, koj tuaj yeem tawm tswv yim rau cov chaw tsim khoom los kho qhov xav tau tshwj xeeb thiab qhov ntau thiab tsawg, uas tuaj yeem ua tau zoo dua rau cov neeg siv khoom siv cov khoom sib txawv.