Aluminium cov pam vov pam vov, tseem hu uaTej ceramic fiber pamCov pam vov pam vov, yog cov ntaub pam vov nyob rau hauv high -}}} pa cov khoom siv kub thiab tsis kam ua cua sov. Txawm li cas los xij, muaj cov sib txawv tseem ceeb ntawm cov txheej txheem alumina silicate pams thiab siab} cov pam vov uas yuav khoom hauv kev lag luam rwb thaiv tsev yuav tsum paub txog.

aluminum silicate needle blanket

1. Tshuaj lom neeg sib xyaw
-} Txheem Txhuas Txhuas Hniav: Feem ntau muaj nyob ib ncig ntawm 46-50% (al₂o₃) thiab 47-52% sillica (sitio₂). Qhov no muaj pes tsawg leeg muab rwb thaiv tsev thermal thiab tiv taus mus rau qhov kub.
High Alumina Wool Pam: muaj qhov siab dua ntawm alumina, feem ntau ntawm 52-55% al₂o₃. Cov ntsiab lus alumina nce ntxiv txhim kho daim pam tsis kam rau qhov kub thiab txias dua thiab tshuaj lom neeg.

2. Thermal Performance
Alumina Silicate Pam-Rwb thaiv tsev: Muaj cov rwb thaiv tsev zoo nrog kev ua haujlwm siab tshaj plaws ntawm ib ncig 1260℃(2300℃f). Nws yog qhov tsim nyog rau cov ntawv thov uas tsis pub dhau qhov kev txwv ntawm Alumina Pam Rwb Thaiv Tsev: Muab cov pa siab zoo dua, txog 1360℃(2480℃f). Qhov no ua rau nws zoo tagnrho rau cov ntawv thov uas xav tau cov cua kub siab dua.

3. Cov Khoom Siv Kho Tshuab
Txheem txhuas cov pam cov pam vov: muaj lub zog tensile ntawm ib ncig 0.04 MPA, uas yog qhov txaus rau cov ntawv thov rwb thaiv tsev feem ntau.
HA Rwb thaiv tsev Pam: Muaj me ntsis siab dua lub zog vim yog cov ntsiab lus alumina nce ntxiv, ua rau nws muaj zog nyob hauv cov kev xav tau ib puag ncig
4. Shrinkage ntawm cua sov
Txheem aluminium silicate phaticate fiber ntau: ua pov thawj ib qho shrinkage ntawm ib ncig -3% thaum rhuab rau 24 teev.
High -} Alumina Pam: qhia tau tias muaj kev ntsws nyob ib ncig ntawm -3% thaum rhuab rau 24 teev, qhia tau tias muaj kev ruaj khov dua.

5. Thov cov xwm txheej
Txheem cov txheej txheem txhuas cov vov vov vov: feem ntau yog siv hauv cov ntaub ntawv hluav taws xob dav dav xws li rwb thaiv tsev cov yeeb nkab, thiab cua sov} up rwb thaiv tsev.
High Alumina Ceramic Fiber Pam: nyiam dua rau cov ntawv thov ntau dua xws li high {0} kev tsim tawm qhov twg kub siab thiab tshuaj lom neeg muaj peev xwm.

To taub txog cov qauv sib txawv ntawm cov txheej txheem thiab qib siab alumina aluminium txhuas cov pam vov yog qhov tseem ceeb rau cov neeg yuav khoom hauv cov rwb thaiv tsev kev lag luam. High {- Cov pam vov pam vov kev ua tau zoo dua, thiab cov tshuaj kub zoo dua, ua rau lawv tsim nyog rau cov ntawv thov. Los ntawm xaiv cov hom uas tsim nyog ntawm alumina fiber ntau pam, cov neeg yuav khoom tuaj yeem txhim kho lawv cov kev ua haujlwm rwb thaiv tsev, txo cov nqi kho mob, thiab txhim kho kev ua haujlwm ntawm kev ua haujlwm.